Mechanical
Yield strength63.1MPasourcetypicalnot given (tensile used)
Ultimate tensile strength63.1MPasourcetypical, peak stress (= stress at yield)23.7MPasourcetypical, stress at break
Flexural strength82.9MPasourcetypical20.2x stronger in bending4.1MPasourcetypical
Elongation at breaknot sourcednot sourced
Young's modulus (stiffness)2.33GPasourcetypical34.8x stiffer0.067GPasourcetypical
Density1,140kg/m³sourcetypical1,220kg/m³sourcetypical
Strength to weight55.4kN·m/kg2.85x higher19.4kN·m/kg
Stiffness to weight2.04MN·m/kg37.2x higher0.0549MN·m/kg
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)not sourced
Shear modulus0.833GPanot sourced
Bulk modulus3.89GPanot sourced
Speed of sound1,430m/s234m/s
Thermal
Thermal conductivity0.33W/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)not sourced
Thermal expansion98–102µm/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 Cnot sourced
100 mm part over a 50 °C swing500µm growthnot sourced
Specific heat1,700J/kg·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)not sourced
Heats up and cools (diffusivity)0.17mm²/snot sourced
Thermal shock resistance53.6W/mnot sourced
Melting point188°Csourcetypical217°Csourcetypical
Glass transition55.1°Csourcetypicalnot sourced
Max service temperature89.2°CsourceHDT 0.455 MPa (printed specimens)1.77x hotter50.3°CsourceHDT 0.455 MPa (printed specimens)
Values forUltimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.Ultimaker TPU 95A, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 29, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic Nylon and Plastic TPU are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic Nylon stronger than Plastic TPU?

Plastic Nylon is stronger: its yield strength is 63.1 MPa against tensile strength 23.7 MPa for Plastic TPU (2.66x).

Which is lighter, Plastic Nylon or Plastic TPU?

Plastic Nylon is lighter: 1,140 kg/m³ against 1,220 kg/m³ for Plastic TPU.

Which is stiffer, Plastic Nylon or Plastic TPU?

Plastic Nylon is stiffer: Young's modulus 2.33 GPa against 0.067 GPa for Plastic TPU, so the same part in Plastic Nylon deflects less under the same load.

Which is lighter for the same job, Plastic Nylon or Plastic TPU?

For the same stiffness or strength: Plastic Nylon is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic NylonPlastic TPU
Stiff rod or tie (tension)lighter37.2x heavier
Stiff beam (bending)lighter6.31x heavier
Stiff panel or platelighter3.49x heavier
Strong rod or tielighter2.85x heavier
Strong beamlighter2.06x heavier
Strong panel or platelighter1.75x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which handles higher temperatures, Plastic Nylon or Plastic TPU?

Plastic Nylon does: 89.2 °C against 50.3 °C for Plastic TPU, both HDT 0.455 MPa (printed specimens).

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonPlastic TPU
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonPlastic TPU
Strength against density

Related comparisons