Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources6 documents: Victrex, Outokumpu, Steel Construction Institute, Carpenter Technology
Plastic PEEK
Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)
Stainless Steel 303
1.4305 / UNS S30300, Outokumpu typical values (hot rolled, solution annealed) from 'Steel Grades, Properties and Global Standards'; max service from Carpenter CarTech 303 datasheet
1
VICTREX PEEK 450G Technical Data SheetVictrexPlastic PEEK · Yield strength: typical, tensile yieldPlastic PEEK · Compressive strength: typical, 23 CPlastic PEEK · Flexural strength: typical, flexural stress at yield, 23 CPlastic PEEK · Elongation at break: typical, at breakPlastic PEEK · Young's modulus (stiffness): typical (nominal)Plastic PEEK · Density: typical (crystalline)Plastic PEEK · Thermal conductivity: typical, average, 23 CPlastic PEEK · Thermal expansion: average of flow/cross-flow, below Tg (<143 C)Plastic PEEK · Melting point: typical, DSCPlastic PEEK · Glass transition: onset (midpoint 150 C)Plastic PEEK · Max service temperature: UL 746B RTI, mechanical strength (continuous use index)
2
Steel Grades, Properties and Global StandardsOutokumpuarchived copyStainless Steel 303 · Yield strength: Outokumpu typical (product P = hot rolled plate, transverse)Stainless Steel 303 · Ultimate tensile strength: Outokumpu typicalStainless Steel 303 · Elongation at break: Outokumpu typical, A5Stainless Steel 303 · Young's modulus (stiffness): at RT (Table 12)Stainless Steel 303 · Density: at RTStainless Steel 303 · Thermal conductivity: at RTStainless Steel 303 · Thermal expansion: mean, 20–100 °CStainless Steel 303 · Specific heat: at RT
3
VICTREX PEEK for Use in Fluid Management (2020)VictrexPlastic PEEK · Poisson's ratio: typical
4
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 303 · Poisson's ratio: design value (structural stainless steels)
5
VICTREX PEEK 450G Technical Data Sheet (2012)Victrexarchived copyPlastic PEEK · Specific heat: typical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)
6
Carpenter Stainless Type 303 Data SheetCarpenter Technologyarchived copyStainless Steel 303 · Max service temperature: continuous, scaling limit
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic PEEK stronger than Stainless Steel 303?
Stainless Steel 303 is stronger: its yield strength is 275 MPa against 98 MPa for Plastic PEEK (2.81x).
Which is lighter, Plastic PEEK or Stainless Steel 303?
Plastic PEEK is lighter: 1,300 kg/m³ against 7,900 kg/m³ for Stainless Steel 303.
Which is stiffer, Plastic PEEK or Stainless Steel 303?
Stainless Steel 303 is stiffer: Young's modulus 200 GPa against 4 GPa for Plastic PEEK, so the same part in Stainless Steel 303 deflects less under the same load.
Which is lighter for the same job, Plastic PEEK or Stainless Steel 303?
For the same stiffness or strength: Plastic PEEK is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 303 is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
Plastic PEEK
Stainless Steel 303
Stiff rod or tie (tension)
8.23x heavier
lighter
Stiff beam (bending)
16% heavier
lighter
Stiff panel or plate
lighter
1.65x heavier
Strong rod or tie
lighter
2.17x heavier
Strong beam
lighter
3.05x heavier
Strong panel or plate
lighter
3.63x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PEEK or Stainless Steel 303?
Stainless Steel 303 stretches further before it breaks: 35% elongation at break against 25% for Plastic PEEK.
Thermal
Which conducts heat better, Plastic PEEK or Stainless Steel 303?
Stainless Steel 303 conducts heat better: 15 W/m·K against 0.29 W/m·K for Plastic PEEK.
Which expands less with temperature?
Stainless Steel 303 expands less: 16 µm/m·K against 55 µm/m·K for Plastic PEEK.