Materials / Compare

Plastic PEEK vs. Wood

Compare Plastic PEEK vs. Wood strength, stiffness, weight and thermal properties.

Change either side
Plastic PEEKBulk polymer (molded or machined)
WoodNatural
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength98MPasourcetypical, tensile yieldnot given (tensile used)
Ultimate tensile strengthnot sourced99MPasourcemodulus of rupture (no direct tensile value)
Compressive strength125MPasourcetypical, 23 C46.6MPasourcecompression parallel to grain (maximum crushing strength), 12% MC
Flexural strength165MPasourcetypical, flexural stress at yield, 23 C99MPasourcemodulus of rupture (static bending), 12% MC
Elongation at break25%sourcetypical, at breaknot sourced
Young's modulus (stiffness)4GPasourcetypical (nominal)12.5GPasourcebending MOE, parallel to grain
Density1,300kg/m³sourcetypical (crystalline)not sourced
Strength to weight75.4kN·m/kgnot sourced
Stiffness to weight3.08MN·m/kgnot sourced
Poisson's ratio0.38sourcetypical0.35sourcemu_LR (red oak group, ~12% MC)
Shear modulus1.45GPa4.63GPa3.19x stiffer in shear
Bulk modulus5.56GPa13.9GPa
Speed of sound1,754m/snot sourced
Thermal
Thermal conductivity0.29W/m·Ksourcetypical, average, 23 C0.18W/m·Ksourceacross grain, 12% MC (Table 4-7, approximate)
Thermal expansion55µm/m·Ksourceaverage of flow/cross-flow, below Tg (<143 C)3.1–4.5µm/m·Ksourceparallel to grain, ovendry wood, range across species
100 mm part over a 50 °C swing275µm growth19µm growth14.5x less
Specific heat2,200J/kg·Ksourcetypical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)1,700J/kg·Ksourcesolid wood (all species), 12% MC, 27 C
Heats up and cools (diffusivity)0.101mm²/snot sourced
Thermal shock resistance80.1W/m244W/m3.04x more resistant
Melting point343°Csourcetypical, DSCnot sourced
Glass transition143°Csourceonset (midpoint 150 C)not sourced
Max service temperature240°CsourceUL 746B RTI, mechanical strength (continuous use index)not sourced
Values forVictrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)Northern red oak (Quercus rubra), clear straight-grained specimens at 12% MC, parallel to grain unless stated; USDA FPL Wood Handbook FPL-GTR-282 (2021) Ch. 4 and Ch. 5

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic PEEK stronger than Wood?

Wood is stronger: its tensile strength is 99 MPa against yield strength 98 MPa for Plastic PEEK (1%).

Which is stiffer, Plastic PEEK or Wood?

Wood is stiffer: Young's modulus 12.5 GPa against 4 GPa for Plastic PEEK, so the same part in Wood deflects less under the same load.

Which conducts heat better, Plastic PEEK or Wood?

Plastic PEEK conducts heat better: 0.29 W/m·K against 0.18 W/m·K for Wood.

Which expands less with temperature?

Wood expands less: 3.8 µm/m·K against 55 µm/m·K for Plastic PEEK.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PEEK
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PEEK
Strength against density