Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 1018 · Young's modulus (stiffness): base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Density: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Poisson's ratio: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Thermal conductivity: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Specific heat: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
4
Eastar Copolyester 6763 Product Data SheetEastmanPlastic PETG · Thermal conductivity: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Thermal expansion: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Specific heat: base material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)
5
S275JR Steel GradeOvakoSteel AISI 1018 · Thermal expansion: base material: unalloyed carbon steel, Ovako family table (S275JR, 'none alloyed structural steels', C <= 0.21%); mean 20-300 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Plastic PETG stronger than Steel AISI 1018?
Steel AISI 1018 is stronger: its yield strength is 372 MPa against 46.2 MPa for Plastic PETG (8.05x).
Which is lighter, Plastic PETG or Steel AISI 1018?
Plastic PETG is lighter: 1,270 kg/m³ against 7,861 kg/m³ for Steel AISI 1018.
Which is stiffer, Plastic PETG or Steel AISI 1018?
Steel AISI 1018 is stiffer: Young's modulus 200 GPa against 1.94 GPa for Plastic PETG, so the same part in Steel AISI 1018 deflects less under the same load.
Which is lighter for the same job, Plastic PETG or Steel AISI 1018?
For the same stiffness or strength: Plastic PETG is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel AISI 1018 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.
Part that must be
Plastic PETG
Steel AISI 1018
Stiff rod or tie (tension)
16.7x heavier
lighter
Stiff beam (bending)
1.64x heavier
lighter
Stiff panel or plate
lighter
32% heavier
Strong rod or tie
30% heavier
lighter
Strong beam
lighter
1.54x heavier
Strong panel or plate
lighter
2.18x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PETG or Steel AISI 1018?
Steel AISI 1018 stretches further before it breaks: 15% elongation at break against 7.6% for Plastic PETG.
Thermal
Which conducts heat better, Plastic PETG or Steel AISI 1018?
Steel AISI 1018 conducts heat better: 51.9 W/m·K against 0.21 W/m·K for Plastic PETG.
Which expands less with temperature?
Steel AISI 1018 expands less: 12 µm/m·K against 51 µm/m·K for Plastic PETG.