Materials / Compare

Plastic PETG vs. Titanium

Compare Plastic PETG vs. Titanium strength, stiffness, weight and thermal properties.

Plastic PETG3D printed (FDM)
TitaniumWrought
MechanicalPlastic PETGTitanium
Yield strength46.2MPa1885MPa219.2x stronger
Ultimate tensile strength46.2MPa1940MPa220.3x stronger
Flexural strength78.9MPa1not sourced
Elongation at break7.6%116%22.11x more ductile
Young's modulus (stiffness)1.94GPa1107–122GPa3
Density1,270kg/m³13.49x lighter4,430kg/m³2
Strength to weight36.4kN·m/kg200kN·m/kg5.49x higher
Stiffness to weight1.53MN·m/kg25.8MN·m/kg16.9x higher
Poisson's rationot sourced0.3422
Shear modulusnot sourced42.7GPa
Bulk modulusnot sourced121GPa
Speed of sound1,236m/s5,084m/s4.11x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PETGTitanium
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PETGTitanium
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic PETGTitanium
Thermal conductivitybase material0.21W/m·K46.6W/m·K331.4x more heat through a fin
Thermal expansionbase material51µm/m·K49µm/m·K35.67x less
100 mm part over a 50 °C swing255µm growth45µm growth5.67x less
Specific heatbase material1,300J/kg·K42.24x higher580J/kg·K3
Heats up and cools (diffusivity)0.127mm²/s2.57mm²/s20.2x faster
Thermal shock resistancenot sourced3,730W/m
Melting pointnot sourcedmelting range1,630–1,650°C2
Glass transition77.4°C1not sourced
Max service temperatureHDT 0.455 MPa76.2°C1400°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic ABSPlastic NylonRubberWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PETGTitanium
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic ABSPlastic NylonWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PETGTitanium
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: UltiMaker, TIMET, Eastman
Plastic PETG
Ultimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022.
Titanium
TIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties
  1. 1
    Ultimaker PETG Technical Data Sheet, v1.00UltiMakerarchived copyPlastic PETG · Yield strength: typicalPlastic PETG · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic PETG · Flexural strength: typicalPlastic PETG · Elongation at break: typicalPlastic PETG · Young's modulus (stiffness): typicalPlastic PETG · Density: typicalPlastic PETG · Glass transition: typicalPlastic PETG · Max service temperature: HDT 0.455 MPa (printed specimens)
  2. 2
    TIMETAL 6-4 PropertiesTIMETarchived copyTitanium · Yield strength: typical, plate (>0.187 in), annealed, 0.2% offsetTitanium · Ultimate tensile strength: typical, plate, annealedTitanium · Elongation at break: typical, in 2 in., plate annealedTitanium · Density: nominalTitanium · Poisson's ratio: mean of TIMET measurementsTitanium · Melting point: melting rangeTitanium · Max service temperature: upper recommended use temperature
  3. 3
    TIMETAL 6-4 Data SheetTIMETarchived copyTitanium · Young's modulus (stiffness): typical range, 20 °CTitanium · Thermal conductivity: typical, 20 °C, mill annealedTitanium · Thermal expansion: typical, mean 0-100 °CTitanium · Specific heat: typical, 20 °C
  4. 4
    Eastar Copolyester 6763 Product Data SheetEastmanPlastic PETG · Thermal conductivity: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Thermal expansion: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Specific heat: base material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Plastic PETG stronger than Titanium?

Titanium is stronger: its yield strength is 885 MPa against 46.2 MPa for Plastic PETG (19.2x).

Which is lighter, Plastic PETG or Titanium?

Plastic PETG is lighter: 1,270 kg/m³ against 4,430 kg/m³ for Titanium.

Which is stiffer, Plastic PETG or Titanium?

Titanium is stiffer: Young's modulus 115 GPa against 1.94 GPa for Plastic PETG, so the same part in Titanium deflects less under the same load.

Which is lighter for the same job, Plastic PETG or Titanium?

For the same stiffness or strength: Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PETGTitanium
Stiff rod or tie (tension)16.9x heavierlighter
Stiff beam (bending)2.2x heavierlighter
Stiff panel or plate12% heavierlighter
Strong rod or tie5.49x heavierlighter
Strong beam2.05x heavierlighter
Strong panel or plate25% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic PETG or Titanium?

Titanium stretches further before it breaks: 16% elongation at break against 7.6% for Plastic PETG.

Thermal

Which conducts heat better, Plastic PETG or Titanium?

Titanium conducts heat better: 6.6 W/m·K against 0.21 W/m·K for Plastic PETG.

Which expands less with temperature?

Titanium expands less: 9 µm/m·K against 51 µm/m·K for Plastic PETG.

Related comparisons