Materials / Compare

Plastic PLA vs. Plastic PMMA

Compare Plastic PLA vs. Plastic PMMA strength, stiffness, weight and thermal properties.

Change either side
Plastic PLA3D printed (FDM)
Plastic PMMABulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength52.5MPasourcetypicalnot given (tensile used)
Ultimate tensile strength52.5MPasourcetypical, peak stress (= stress at yield)80MPasourcetypical, 23 °C
Compressive strengthnot sourced110MPasourcecompressive yield stress, typical
Flexural strength96.8MPasourcetypical115MPasourcetypical19% stronger in bending
Elongation at break7.8%sourcetypical42% more ductile5.5%sourcetypical
Young's modulus (stiffness)3.25GPasourcetypical3.3GPasourcetypical, short-term
Density1,240kg/m³sourcetypical1,190kg/m³sourcetypical
Strength to weight42.3kN·m/kg67.2kN·m/kg1.59x higher
Stiffness to weight2.62MN·m/kg2.77MN·m/kg6% higher
Poisson's rationot sourced0.37sourcetypical
Shear modulusnot sourced1.2GPa
Bulk modulusnot sourced4.23GPa
Speed of sound1,619m/s1,665m/s
Thermal
Thermal conductivity0.13W/m·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C0.19W/m·Ksourcetypical
Thermal expansionnot sourced70µm/m·Ksource0-50 °C
100 mm part over a 50 °C swingnot sourced350µm growth
Specific heat1,200J/kg·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C1,470J/kg·Ksourcetypical
Heats up and cools (diffusivity)0.0874mm²/s0.109mm²/s24% faster
Thermal shock resistancenot sourced41.5W/m
Melting point152°Csourcetypicalnot sourced
Glass transition59.1°Csourcetypicalnot sourced
Max service temperature58.8°CsourceHDT 0.455 MPa (printed specimens)80°Csourcemax. permanent service temperature
Values forUltimaker PLA, 3D-printed specimens, XY (flat) orientation; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS dated April 20, 2022.Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PLA is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic PLA stronger than Plastic PMMA?

Plastic PMMA is stronger: its tensile strength is 80 MPa against yield strength 52.5 MPa for Plastic PLA (1.52x).

Which is lighter, Plastic PLA or Plastic PMMA?

Plastic PMMA is lighter: 1,190 kg/m³ against 1,240 kg/m³ for Plastic PLA.

Which is stiffer, Plastic PLA or Plastic PMMA?

Plastic PMMA is stiffer: Young's modulus 3.3 GPa against 3.25 GPa for Plastic PLA, so the same part in Plastic PMMA deflects less under the same load.

Which is lighter for the same job, Plastic PLA or Plastic PMMA?

For the same stiffness or strength: Plastic PMMA is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PLAPlastic PMMA
Stiff rod or tie (tension)6% heavierlighter
Stiff beam (bending)5% heavierlighter
Stiff panel or plate5% heavierlighter
Strong rod or tie1.59x heavierlighter
Strong beam38% heavierlighter
Strong panel or plate29% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic PLA or Plastic PMMA?

Plastic PLA stretches further before it breaks: 7.8% elongation at break against 5.5% for Plastic PMMA.

Which conducts heat better, Plastic PLA or Plastic PMMA?

Plastic PMMA conducts heat better: 0.19 W/m·K against 0.13 W/m·K for Plastic PLA.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PLAPlastic PMMA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PLAPlastic PMMA
Strength against density

Related comparisons