Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values
SLA Resin Elastic 50A
Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.
1
Makrolon 2405 Technical Data SheetCovestroPlastic Polycarbonate · Yield strength: typical, tensile yieldPlastic Polycarbonate · Ultimate tensile strength: typical, stress at breakPlastic Polycarbonate · Flexural strength: typical, flexural strengthPlastic Polycarbonate · Elongation at break: typical, strain at breakPlastic Polycarbonate · Young's modulus (stiffness): typicalPlastic Polycarbonate · Density: typicalPlastic Polycarbonate · Thermal conductivity: typical, through-plane, 23 CPlastic Polycarbonate · Thermal expansion: typical, 23-55 C, parallel and normalPlastic Polycarbonate · Glass transition: typical, DSC 10 C/minPlastic Polycarbonate · Max service temperature: UL 746B RTI, tensile strength, 1.5 mm
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
4
Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Plastic Polycarbonate stronger than SLA Resin Elastic 50A?
Plastic Polycarbonate is stronger: its yield strength is 65 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (19.1x).
Which is lighter, Plastic Polycarbonate or SLA Resin Elastic 50A?
SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 1,200 kg/m³ for Plastic Polycarbonate.
Which is lighter for the same job, Plastic Polycarbonate or SLA Resin Elastic 50A?
For the same stiffness or strength: Plastic Polycarbonate is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Plastic Polycarbonate
SLA Resin Elastic 50A
Strong rod or tie
lighter
16.1x heavier
Strong beam
lighter
6.02x heavier
Strong panel or plate
lighter
3.68x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic Polycarbonate or SLA Resin Elastic 50A?
SLA Resin Elastic 50A stretches further before it breaks: 160% elongation at break against 125% for Plastic Polycarbonate.