Materials / Compare

Plastic Polycarbonate vs. Stainless Steel 17-4PH

Compare Plastic Polycarbonate vs. Stainless Steel 17-4PH strength, stiffness, weight and thermal properties.

Plastic PolycarbonateBulk polymer (molded or machined)
Stainless Steel 17-4PHWrought
MechanicalPlastic PolycarbonateStainless Steel 17-4PH
Yield strength65MPa11,275MPa219.6x stronger
Ultimate tensile strength65MPa11,379MPa2
Flexural strength97MPa1not sourced
Elongation at break125%113.9x more ductile9%2
Young's modulus (stiffness)2.4GPa1H 900197GPa282.1x stiffer
Density1,200kg/m³16.5x lighterH 9007,800kg/m³2
Strength to weight54.2kN·m/kg163kN·m/kg3.02x higher
Stiffness to weight2MN·m/kg25.3MN·m/kg12.6x higher
Poisson's ratio0.383H 9000.2722
Shear modulus0.87GPa77.4GPa89.1x stiffer in shear
Bulk modulus3.33GPa144GPa43.2x higher
Speed of sound1,414m/s5,026m/s3.55x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PolycarbonateStainless Steel 17-4PH
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PolycarbonateStainless Steel 17-4PH
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic PolycarbonateStainless Steel 17-4PH
Thermal conductivity0.2W/m·K1at 149 °C17.9W/m·K289.5x more heat through a fin
Thermal expansion65µm/m·K1mean10.8µm/m·K26.02x less
100 mm part over a 50 °C swing325µm growth54µm growth6.02x less
Specific heat1,172J/kg·K42.55x highermean460J/kg·K2
Heats up and cools (diffusivity)0.142mm²/s4.99mm²/s35.1x faster
Thermal shock resistance51.7W/m7,809W/m151x more resistant
Glass transition144°C1not sourced
Max service temperatureUL 746B RTI125°C1316°C2191 °C hotter
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PolycarbonateStainless Steel 17-4PH
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PolycarbonateStainless Steel 17-4PH
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Covestro, Cleveland-Cliffs, Bayer MaterialScience
Plastic Polycarbonate
Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values
Stainless Steel 17-4PH
Cleveland-Cliffs 17-4 PH, Condition H 900, sheet/strip, transverse (Product Data Bulletin, May 2021)
  1. 1
    Makrolon 2405 Technical Data SheetCovestroPlastic Polycarbonate · Yield strength: typical, tensile yieldPlastic Polycarbonate · Ultimate tensile strength: typical, stress at breakPlastic Polycarbonate · Flexural strength: typical, flexural strengthPlastic Polycarbonate · Elongation at break: typical, strain at breakPlastic Polycarbonate · Young's modulus (stiffness): typicalPlastic Polycarbonate · Density: typicalPlastic Polycarbonate · Thermal conductivity: typical, through-plane, 23 CPlastic Polycarbonate · Thermal expansion: typical, 23-55 C, parallel and normalPlastic Polycarbonate · Glass transition: typical, DSC 10 C/minPlastic Polycarbonate · Max service temperature: UL 746B RTI, tensile strength, 1.5 mm
  2. 2
    17-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 17-4PH · Yield strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Ultimate tensile strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Elongation at break: typical, transverse, in 2 in. (50.8 mm)Stainless Steel 17-4PH · Young's modulus (stiffness): H 900Stainless Steel 17-4PH · Density: H 900Stainless Steel 17-4PH · Poisson's ratio: H 900 (column)Stainless Steel 17-4PH · Thermal conductivity: at 149 °C (300 °F), H 900Stainless Steel 17-4PH · Thermal expansion: mean, 21–93 °C (70–200 °F), H 900Stainless Steel 17-4PH · Specific heat: mean, 0–100 °C, H 900Stainless Steel 17-4PH · Max service temperature: strength-retention limit (not oxidation)
  3. 3
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
  4. 4
    Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Plastic Polycarbonate stronger than Stainless Steel 17-4PH?

Stainless Steel 17-4PH is stronger: its yield strength is 1,275 MPa against 65 MPa for Plastic Polycarbonate (19.6x).

Which is lighter, Plastic Polycarbonate or Stainless Steel 17-4PH?

Plastic Polycarbonate is lighter: 1,200 kg/m³ against 7,800 kg/m³ for Stainless Steel 17-4PH.

Which is stiffer, Plastic Polycarbonate or Stainless Steel 17-4PH?

Stainless Steel 17-4PH is stiffer: Young's modulus 197 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Stainless Steel 17-4PH deflects less under the same load.

Which is lighter for the same job, Plastic Polycarbonate or Stainless Steel 17-4PH?

For the same stiffness or strength: Plastic Polycarbonate is lighter for a stiff panel or plate, strong panel or plate; Stainless Steel 17-4PH is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam.

Part that must bePlastic PolycarbonateStainless Steel 17-4PH
Stiff rod or tie (tension)12.6x heavierlighter
Stiff beam (bending)39% heavierlighter
Stiff panel or platelighter50% heavier
Strong rod or tie3.02x heavierlighter
Strong beam12% heavierlighter
Strong panel or platelighter47% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic Polycarbonate or Stainless Steel 17-4PH?

Plastic Polycarbonate stretches further before it breaks: 125% elongation at break against 9% for Stainless Steel 17-4PH.

Thermal

Which handles higher temperatures, Plastic Polycarbonate or Stainless Steel 17-4PH?

Stainless Steel 17-4PH does: 316 °C against 125 °C for Plastic Polycarbonate.

Which conducts heat better, Plastic Polycarbonate or Stainless Steel 17-4PH?

Stainless Steel 17-4PH conducts heat better: 17.9 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.

Which expands less with temperature?

Stainless Steel 17-4PH expands less: 10.8 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.

Related comparisons