Materials / Compare
Plastic Polycarbonate vs. Stainless Steel 304
Compare Plastic Polycarbonate vs. Stainless Steel 304 strength, stiffness, weight and thermal properties.
| Mechanical | Plastic Polycarbonate | Stainless Steel 304 |
|---|---|---|
| Yield strength | 65MPa1 | 241MPa23.71x stronger |
| Ultimate tensile strength | 65MPa1 | 586MPa2 |
| Flexural strength | 97MPa1 | not sourced |
| Elongation at break | 125%12.27x more ductile | 55%2 |
| Young's modulus (stiffness) | 2.4GPa1 | 193GPa280.4x stiffer |
| Density | 1,200kg/m³16.69x lighter | 8,030kg/m³2 |
| Strength to weight | 54.2kN·m/kg1.8x higher | 30kN·m/kg |
| Stiffness to weight | 2MN·m/kg | 24MN·m/kg12x higher |
| Poisson's ratio | 0.383 | design value0.34 |
| Shear modulus | 0.87GPa | 74.2GPa85.4x stiffer in shear |
| Bulk modulus | 3.33GPa | 161GPa48.2x higher |
| Speed of sound | 1,414m/s | 4,903m/s3.47x faster |
| Thermal | Plastic Polycarbonate | Stainless Steel 304 |
|---|---|---|
| Thermal conductivity | 0.2W/m·K1 | at 100 °C16.2W/m·K281x more heat through a fin |
| Thermal expansion | 65µm/m·K1 | mean16.9µm/m·K23.85x less |
| 100 mm part over a 50 °C swing | 325µm growth | 84.5µm growth3.85x less |
| Specific heat | 1,172J/kg·K52.34x higher | mean500J/kg·K2 |
| Heats up and cools (diffusivity) | 0.142mm²/s | 4.03mm²/s28.4x faster |
| Thermal shock resistance | 51.7W/m | 838W/m16.2x more resistant |
| Melting point | not sourced | melting range1,399–1,454°C2 |
| Glass transition | 144°C1 | not sourced |
| Max service temperature | UL 746B RTI125°C1 | continuous899°C2774 °C hotter |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources5 documents: Covestro, Cleveland-Cliffs, Steel Construction Institute, Bayer MaterialScience
- Plastic Polycarbonate
- Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values
- Stainless Steel 304
- Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
- 1Makrolon 2405 Technical Data SheetCovestroPlastic Polycarbonate · Yield strength: typical, tensile yieldPlastic Polycarbonate · Ultimate tensile strength: typical, stress at breakPlastic Polycarbonate · Flexural strength: typical, flexural strengthPlastic Polycarbonate · Elongation at break: typical, strain at breakPlastic Polycarbonate · Young's modulus (stiffness): typicalPlastic Polycarbonate · Density: typicalPlastic Polycarbonate · Thermal conductivity: typical, through-plane, 23 CPlastic Polycarbonate · Thermal expansion: typical, 23-55 C, parallel and normalPlastic Polycarbonate · Glass transition: typical, DSC 10 C/minPlastic Polycarbonate · Max service temperature: UL 746B RTI, tensile strength, 1.5 mm
- 2304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
- 3Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
- 4Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)
- 5Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic Polycarbonate stronger than Stainless Steel 304?
Stainless Steel 304 is stronger: its yield strength is 241 MPa against 65 MPa for Plastic Polycarbonate (3.71x).
Which is lighter, Plastic Polycarbonate or Stainless Steel 304?
Plastic Polycarbonate is lighter: 1,200 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.
Which is stiffer, Plastic Polycarbonate or Stainless Steel 304?
Stainless Steel 304 is stiffer: Young's modulus 193 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Stainless Steel 304 deflects less under the same load.
Which is lighter for the same job, Plastic Polycarbonate or Stainless Steel 304?
For the same stiffness or strength: Plastic Polycarbonate is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 304 is lighter for a stiff rod or tie (tension), stiff beam (bending).
| Part that must be | Plastic Polycarbonate | Stainless Steel 304 |
|---|---|---|
| Stiff rod or tie (tension) | 12x heavier | lighter |
| Stiff beam (bending) | 34% heavier | lighter |
| Stiff panel or plate | lighter | 1.55x heavier |
| Strong rod or tie | lighter | 1.8x heavier |
| Strong beam | lighter | 2.79x heavier |
| Strong panel or plate | lighter | 3.48x heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic Polycarbonate or Stainless Steel 304?
Plastic Polycarbonate stretches further before it breaks: 125% elongation at break against 55% for Stainless Steel 304.
Thermal
Which handles higher temperatures, Plastic Polycarbonate or Stainless Steel 304?
Stainless Steel 304 does: 899 °C against 125 °C for Plastic Polycarbonate.
Which conducts heat better, Plastic Polycarbonate or Stainless Steel 304?
Stainless Steel 304 conducts heat better: 16.2 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.
Which expands less with temperature?
Stainless Steel 304 expands less: 16.9 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.
Related comparisons
- Plastic Polycarbonate vs. Plastic Nylon
- Plastic Polycarbonate vs. SLA Resin Standard
- Plastic Polycarbonate vs. FDM Polycarbonate
- Plastic Polycarbonate vs. Plastic POM/Acetal
- Stainless Steel 304 vs. Stainless Steel 316
- Stainless Steel 304 vs. Stainless Steel 303
- Stainless Steel 304 vs. Iron
- Stainless Steel 304 vs. Steel AISI 1018