| Mechanical | Plastic Polycarbonate | Stainless Steel 316 |
|---|---|---|
| Yield strength | 65MPa1 | 265MPa24.08x stronger |
| Ultimate tensile strength | 65MPa1 | 583MPa2 |
| Flexural strength | 97MPa1 | not sourced |
| Elongation at break | 125%12.05x more ductile | 61%2 |
| Young's modulus (stiffness) | 2.4GPa1 | 200GPa283.3x stiffer |
| Density | 1,200kg/m³16.69x lighter | 8,027kg/m³2 |
| Strength to weight | 54.2kN·m/kg1.64x higher | 33kN·m/kg |
| Stiffness to weight | 2MN·m/kg | 24.9MN·m/kg12.5x higher |
| Poisson's ratio | 0.383 | design value0.34 |
| Shear modulus | 0.87GPa | 76.9GPa88.5x stiffer in shear |
| Bulk modulus | 3.33GPa | 167GPa50x higher |
| Speed of sound | 1,414m/s | 4,992m/s3.53x faster |
| Thermal | Plastic Polycarbonate | Stainless Steel 316 |
|---|---|---|
| Thermal conductivity | 0.2W/m·K1 | 20–100 °C14.6W/m·K273x more heat through a fin |
| Thermal expansion | 65µm/m·K1 | mean16.5µm/m·K23.94x less |
| 100 mm part over a 50 °C swing | 325µm growth | 82.5µm growth3.94x less |
| Specific heat | 1,172J/kg·K52.6x higher | at 20 °C450J/kg·K2 |
| Heats up and cools (diffusivity) | 0.142mm²/s | 4.04mm²/s28.4x faster |
| Thermal shock resistance | 51.7W/m | 821W/m15.9x more resistant |
| Melting point | not sourced | melting range1,390–1,440°C2 |
| Glass transition | 144°C1 | not sourced |
| Max service temperature | UL 746B RTI125°C1 | oxidation871–899°C2 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources5 documents: Covestro, ATI, Steel Construction Institute, Bayer MaterialScience
- Plastic Polycarbonate
- Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values
- Stainless Steel 316
- ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
- 1Makrolon 2405 Technical Data SheetCovestroPlastic Polycarbonate · Yield strength: typical, tensile yieldPlastic Polycarbonate · Ultimate tensile strength: typical, stress at breakPlastic Polycarbonate · Flexural strength: typical, flexural strengthPlastic Polycarbonate · Elongation at break: typical, strain at breakPlastic Polycarbonate · Young's modulus (stiffness): typicalPlastic Polycarbonate · Density: typicalPlastic Polycarbonate · Thermal conductivity: typical, through-plane, 23 CPlastic Polycarbonate · Thermal expansion: typical, 23-55 C, parallel and normalPlastic Polycarbonate · Glass transition: typical, DSC 10 C/minPlastic Polycarbonate · Max service temperature: UL 746B RTI, tensile strength, 1.5 mm
- 2ATI 316, 316L, 317 and 317L Technical Data Sheet (2012)ATIarchived copyStainless Steel 316 · Yield strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Ultimate tensile strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Elongation at break: typical (representative), annealed, in 2 in. (51 mm)Stainless Steel 316 · Young's modulus (stiffness): typical, in tensionStainless Steel 316 · Density: typicalStainless Steel 316 · Thermal conductivity: 20–100 °CStainless Steel 316 · Thermal expansion: mean, 20–100 °CStainless Steel 316 · Specific heat: at 20 °CStainless Steel 316 · Melting point: melting rangeStainless Steel 316 · Max service temperature: oxidation (scaling) limit in air
- 3Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
- 4Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)
- 5Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic Polycarbonate stronger than Stainless Steel 316?
Stainless Steel 316 is stronger: its yield strength is 265 MPa against 65 MPa for Plastic Polycarbonate (4.08x).
Which is lighter, Plastic Polycarbonate or Stainless Steel 316?
Plastic Polycarbonate is lighter: 1,200 kg/m³ against 8,027 kg/m³ for Stainless Steel 316.
Which is stiffer, Plastic Polycarbonate or Stainless Steel 316?
Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Stainless Steel 316 deflects less under the same load.
Which is lighter for the same job, Plastic Polycarbonate or Stainless Steel 316?
For the same stiffness or strength: Plastic Polycarbonate is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 316 is lighter for a stiff rod or tie (tension), stiff beam (bending).
| Part that must be | Plastic Polycarbonate | Stainless Steel 316 |
|---|---|---|
| Stiff rod or tie (tension) | 12.5x heavier | lighter |
| Stiff beam (bending) | 36% heavier | lighter |
| Stiff panel or plate | lighter | 1.53x heavier |
| Strong rod or tie | lighter | 1.64x heavier |
| Strong beam | lighter | 2.62x heavier |
| Strong panel or plate | lighter | 3.31x heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic Polycarbonate or Stainless Steel 316?
Plastic Polycarbonate stretches further before it breaks: 125% elongation at break against 61% for Stainless Steel 316.
Thermal
Which conducts heat better, Plastic Polycarbonate or Stainless Steel 316?
Stainless Steel 316 conducts heat better: 14.6 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.
Which expands less with temperature?
Stainless Steel 316 expands less: 16.5 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.
Related comparisons
- Plastic Polycarbonate vs. Plastic Nylon
- Plastic Polycarbonate vs. SLA Resin Standard
- Plastic Polycarbonate vs. FDM Polycarbonate
- Plastic Polycarbonate vs. Plastic POM/Acetal
- Stainless Steel 316 vs. Stainless Steel 303
- Stainless Steel 316 vs. Stainless Steel 304
- Stainless Steel 316 vs. Steel AISI 1018
- Stainless Steel 316 vs. Iron