Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources7 documents: Covestro, American Institute of Steel Construction, bauforumstahl (ArcelorMittal), Bayer MaterialScience, Ovako
Plastic Polycarbonate
Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values
Steel
Generic structural steel, cited as ASTM A992 (the current US structural grade): ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
1
Makrolon 2405 Technical Data SheetCovestroPlastic Polycarbonate · Yield strength: typical, tensile yieldPlastic Polycarbonate · Ultimate tensile strength: typical, stress at breakPlastic Polycarbonate · Flexural strength: typical, flexural strengthPlastic Polycarbonate · Elongation at break: typical, strain at breakPlastic Polycarbonate · Young's modulus (stiffness): typicalPlastic Polycarbonate · Density: typicalPlastic Polycarbonate · Thermal conductivity: typical, through-plane, 23 CPlastic Polycarbonate · Thermal expansion: typical, 23-55 C, parallel and normalPlastic Polycarbonate · Glass transition: typical, DSC 10 C/minPlastic Polycarbonate · Max service temperature: UL 746B RTI, tensile strength, 1.5 mm
2
Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
3
ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel · Young's modulus (stiffness): design value (AISC 360-16)Steel · Poisson's ratio: design value (AISC 360-16 Commentary)
4
Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel · Density: nominal (constructional data)Steel · Thermal conductivity: nominal at 20 °CSteel · Thermal expansion: nominal (constructional data, no temperature range stated)
5
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
6
Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
7
S275JR Steel GradeOvakoSteel · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic Polycarbonate stronger than Steel?
Steel is stronger: its yield strength is 385 MPa against 65 MPa for Plastic Polycarbonate (5.92x).
Which is lighter, Plastic Polycarbonate or Steel?
Plastic Polycarbonate is lighter: 1,200 kg/m³ against 7,850 kg/m³ for Steel.
Which is stiffer, Plastic Polycarbonate or Steel?
Steel is stiffer: Young's modulus 200 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Steel deflects less under the same load.
Which is lighter for the same job, Plastic Polycarbonate or Steel?
For the same stiffness or strength: Plastic Polycarbonate is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Steel is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
Plastic Polycarbonate
Steel
Stiff rod or tie (tension)
12.7x heavier
lighter
Stiff beam (bending)
40% heavier
lighter
Stiff panel or plate
lighter
50% heavier
Strong rod or tie
lighter
10% heavier
Strong beam
lighter
2x heavier
Strong panel or plate
lighter
2.69x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic Polycarbonate or Steel?
Plastic Polycarbonate stretches further before it breaks: 125% elongation at break against 24.2% for Steel.
Thermal
Which conducts heat better, Plastic Polycarbonate or Steel?
Steel conducts heat better: 48 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.
Which expands less with temperature?
Steel expands less: 12 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.