Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Chemours, Cleveland-Cliffs, Steel Construction Institute
Plastic PTFE
Chemours Teflon PTFE 7C X granular molding resin, typical values (tensile/elongation measured on 0.13 mm skived tape)
Stainless Steel 304
Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
1
Teflon PTFE Fluoropolymer Resin Properties HandbookChemoursarchived copyPlastic PTFE · Yield strength: typical yield strength at 23 °C (Teflon PTFE, Table 8)Plastic PTFE · Poisson's ratio: typical, 23 °C (Teflon PTFE resins, Chemours handbook)Plastic PTFE · Thermal conductivity: typical, granular resin, 4.6 mm specimenPlastic PTFE · Thermal expansion: typical, granular resin, 23-60 °C (ASTM E228)Plastic PTFE · Specific heat: typical, granular resin, 20 °C (ASTM D4591)
2
304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)
5
Teflon PTFE 6C X Product InformationChemoursarchived copyPlastic PTFE · Max service temperature: service temperature (Chemours general Teflon PTFE statement)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic PTFE stronger than Stainless Steel 304?
Stainless Steel 304 is stronger: its yield strength is 241 MPa against 9 MPa for Plastic PTFE (26.8x).
Which is lighter, Plastic PTFE or Stainless Steel 304?
Plastic PTFE is lighter: 2,160 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.
Which is lighter for the same job, Plastic PTFE or Stainless Steel 304?
For the same stiffness or strength: Stainless Steel 304 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Plastic PTFE
Stainless Steel 304
Strong rod or tie
7.2x heavier
lighter
Strong beam
2.41x heavier
lighter
Strong panel or plate
39% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PTFE or Stainless Steel 304?
Plastic PTFE stretches further before it breaks: 350% elongation at break against 55% for Stainless Steel 304.
Thermal
Which conducts heat better, Plastic PTFE or Stainless Steel 304?
Stainless Steel 304 conducts heat better: 16.2 W/m·K against 0.25 W/m·K for Plastic PTFE.
Which expands less with temperature?
Stainless Steel 304 expands less: 16.9 µm/m·K against 100 µm/m·K for Plastic PTFE.