Materials / Compare

Plastic PTFE vs. Zinc Zamak 3

Compare Plastic PTFE vs. Zinc Zamak 3 strength, stiffness, weight and thermal properties.

Plastic PTFEBulk polymer (molded or machined)
Zinc Zamak 3Cast
MechanicalPlastic PTFEZinc Zamak 3
Yield strength9MPa1221MPa224.6x stronger
Ultimate tensile strength39.3MPa3283MPa27.2x stronger
Elongation at break350%335x more ductile10%2
Young's modulus (stiffness)not sourced85.5GPa2
Density2,160kg/m³33.06x lighter6,600kg/m³2
Strength to weight4.17kN·m/kg33.5kN·m/kg8.04x higher
Stiffness to weightnot sourced13MN·m/kg
Poisson's ratio0.4610.274
Shear modulusnot sourced33.7GPa
Bulk modulusnot sourced62GPa
Speed of soundnot sourced3,599m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Zinc Zamak 3
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PTFEZinc Zamak 3
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic PTFEZinc Zamak 3
Thermal conductivity0.25W/m·K1113W/m·K2452x more heat through a fin
Thermal expansion100µm/m·K127.4µm/m·K23.65x less
100 mm part over a 50 °C swing500µm growth137µm growth3.65x less
Specific heat1,400J/kg·K13.34x higher419J/kg·K2
Heats up and cools (diffusivity)0.0827mm²/s40.9mm²/s495x faster
Thermal shock resistancenot sourced7,782W/m
Melting pointsecond melting peak327°C3melting range381–387°C2
Max service temperatureservice temperature260°C5not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PTFEZinc Zamak 3
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PTFEZinc Zamak 3
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Chemours, Nathan Trotter, Eastern Alloys
Plastic PTFE
Chemours Teflon PTFE 7C X granular molding resin, typical values (tensile/elongation measured on 0.13 mm skived tape)
Zinc Zamak 3
Zamak 3 (ASTM B86 die cast), Nathan Trotter (zinc alloy producer) technical data sheet, typical values
  1. 1
    Teflon PTFE Fluoropolymer Resin Properties HandbookChemoursarchived copyPlastic PTFE · Yield strength: typical yield strength at 23 °C (Teflon PTFE, Table 8)Plastic PTFE · Poisson's ratio: typical, 23 °C (Teflon PTFE resins, Chemours handbook)Plastic PTFE · Thermal conductivity: typical, granular resin, 4.6 mm specimenPlastic PTFE · Thermal expansion: typical, granular resin, 23-60 °C (ASTM E228)Plastic PTFE · Specific heat: typical, granular resin, 20 °C (ASTM D4591)
  2. 2
    Zamak 3 Technical Data SheetNathan Trotterarchived copyZinc Zamak 3 · Yield strength: typicalZinc Zamak 3 · Ultimate tensile strength: typicalZinc Zamak 3 · Elongation at break: typical, in 2 in.Zinc Zamak 3 · Young's modulus (stiffness): typicalZinc Zamak 3 · Density: typicalZinc Zamak 3 · Thermal conductivity: typicalZinc Zamak 3 · Thermal expansion: typicalZinc Zamak 3 · Specific heat: typicalZinc Zamak 3 · Melting point: melting range
  3. 3
    Teflon PTFE 7C X Product InformationChemoursarchived copyPlastic PTFE · Ultimate tensile strength: typical, skived tape 0.13 mmPlastic PTFE · Elongation at break: typical, skived tape 0.13 mmPlastic PTFE · Density: typical (standard specific gravity, ASTM D4894)Plastic PTFE · Melting point: second melting peak (sintered polymer), +/-10
  4. 4
    Zinc Die Casting Properties Guide (2012)Eastern AlloysZinc Zamak 3 · Poisson's ratio: typical, Zamak 3 hot-chamber die cast
  5. 5
    Teflon PTFE 6C X Product InformationChemoursarchived copyPlastic PTFE · Max service temperature: service temperature (Chemours general Teflon PTFE statement)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Plastic PTFE stronger than Zinc Zamak 3?

Zinc Zamak 3 is stronger: its yield strength is 221 MPa against 9 MPa for Plastic PTFE (24.6x).

Which is lighter, Plastic PTFE or Zinc Zamak 3?

Plastic PTFE is lighter: 2,160 kg/m³ against 6,600 kg/m³ for Zinc Zamak 3.

Which is lighter for the same job, Plastic PTFE or Zinc Zamak 3?

For the same stiffness or strength: Zinc Zamak 3 is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PTFEZinc Zamak 3
Strong rod or tie8.04x heavierlighter
Strong beam2.76x heavierlighter
Strong panel or plate1.62x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic PTFE or Zinc Zamak 3?

Plastic PTFE stretches further before it breaks: 350% elongation at break against 10% for Zinc Zamak 3.

Thermal

Which conducts heat better, Plastic PTFE or Zinc Zamak 3?

Zinc Zamak 3 conducts heat better: 113 W/m·K against 0.25 W/m·K for Plastic PTFE.

Which expands less with temperature?

Zinc Zamak 3 expands less: 27.4 µm/m·K against 100 µm/m·K for Plastic PTFE.

Related comparisons