Materials / Compare

Plywood vs. Stainless Steel 316

Compare Plywood vs. Stainless Steel 316 strength, stiffness, weight and thermal properties.

PlywoodNatural
Stainless Steel 316Wrought
MechanicalPlywoodStainless Steel 316
Yield strengthnot given (tensile used)265MPa1
Ultimate tensile strengthmodulus of rupture41.4MPa2583MPa1
Flexural strengthstatic bending MOR41.4MPa2not sourced
Elongation at breaknot sourced61%1
Young's modulus (stiffness)7.45GPa2200GPa126.8x stiffer
Densitynot sourced8,027kg/m³1
Strength to weightnot sourced33kN·m/kg
Stiffness to weightnot sourced24.9MN·m/kg
Poisson's rationot sourceddesign value0.33
Shear modulusnot sourced76.9GPa
Bulk modulusnot sourced167GPa
Speed of soundnot sourced4,992m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Stainless Steel 316
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Stainless Steel 316
Strength against densityHigher and further left: stronger for its weight
ThermalPlywoodStainless Steel 316
Thermal conductivity0.12W/m·K420–100 °C14.6W/m·K1
Thermal expansionbase material3.1–4.5µm/m·K5mean16.5µm/m·K1
100 mm part over a 50 °C swing19µm growth4.34x less82.5µm growth
Specific heatbase material1,700J/kg·K53.78x higherat 20 °C450J/kg·K1
Heats up and cools (diffusivity)not sourced4.04mm²/s
Thermal shock resistancenot sourced821W/m
Melting pointnot sourcedmelting range1,390–1,440°C1
Max service temperaturenot sourcedoxidation871–899°C1
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Stainless Steel 316
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30PlywoodStainless Steel 316
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: ATI, USDA Forest Products Laboratory, Steel Construction Institute
Plywood
Douglas-fir plywood sheathing (construction plywood per PS 1), static bending properties from USDA FPL Wood Handbook FPL-GTR-282 Ch. 12 Table 12-2 (Biblis 2000)
Stainless Steel 316
ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
  1. 1
    ATI 316, 316L, 317 and 317L Technical Data Sheet (2012)ATIarchived copyStainless Steel 316 · Yield strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Ultimate tensile strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Elongation at break: typical (representative), annealed, in 2 in. (51 mm)Stainless Steel 316 · Young's modulus (stiffness): typical, in tensionStainless Steel 316 · Density: typicalStainless Steel 316 · Thermal conductivity: 20–100 °CStainless Steel 316 · Thermal expansion: mean, 20–100 °CStainless Steel 316 · Specific heat: at 20 °CStainless Steel 316 · Melting point: melting rangeStainless Steel 316 · Max service temperature: oxidation (scaling) limit in air
  2. 2
    Wood Handbook (FPL-GTR-282), Chapter 12: Mechanical Properties of Wood-Based Composite MaterialsUSDA Forest Products LaboratoryPlywood · Ultimate tensile strength: modulus of rupture (no direct tensile value)Plywood · Flexural strength: static bending MOR (Douglas-fir); range 33.72-42.61 across speciesPlywood · Young's modulus (stiffness): static bending MOE of the panel (Douglas-fir); range 6.96-8.55 across species
  3. 3
    Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)
  4. 4
    Thermal Properties of Wood and Wood Panel Products for Use in Buildings (1988)USDA Forest Products Laboratoryarchived copyPlywood · Thermal conductivity: APA-recommended design value (Douglas-fir plywood), as reported by FPL/ORNL
  5. 5
    Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of WoodUSDA Forest Products LaboratoryPlywood · Thermal expansion: base material: solid wood parallel to grain, ovendry, range across speciesPlywood · Specific heat: base material: solid wood (all species), 12% MC, 27 C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Plywood stronger than Stainless Steel 316?

Stainless Steel 316 is stronger: its yield strength is 265 MPa against tensile strength 41.4 MPa for Plywood (6.41x).

Which is stiffer, Plywood or Stainless Steel 316?

Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 7.45 GPa for Plywood, so the same part in Stainless Steel 316 deflects less under the same load.

Thermal

Which conducts heat better, Plywood or Stainless Steel 316?

Stainless Steel 316 conducts heat better: 14.6 W/m·K against 0.12 W/m·K for Plywood.

Which expands less with temperature?

Plywood expands less: 3.8 µm/m·K against 16.5 µm/m·K for Stainless Steel 316.