Materials / Compare

Plastic Polypropylene vs. DMLS Ti-6Al-4V ELI Titanium

Compare Plastic Polypropylene vs. DMLS Ti-6Al-4V ELI Titanium strength, stiffness, weight and thermal properties.

Change either side
Plastic PolypropyleneBulk polymer (molded or machined)
DMLS Ti-6Al-4V ELI Titanium3D printed metal (DMLS)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength33MPasourcetypical, tensile stress at yield ISO 5271,100MPasourcetypical, as built, average of horizontal + vertical (M400)
Ultimate tensile strengthnot sourced1,270MPasourcetypical, as built, average of horizontal + vertical (M400)
Elongation at breaknot sourced8.7%sourcetypical at break, as built (M400)
Young's modulus (stiffness)1.45GPasourcetypical, tensile modulus ISO 527110GPasourcesame maker and process, sibling grade: EOS Titanium Ti64 (Grade 5) on EOS M 290, as built, XY and Z, typical
Density900kg/m³sourcetypical, 23 °C ISO 1183-14,400kg/m³sourcetypical part density (ISO 3369), M400
Strength to weight36.7kN·m/kg250kN·m/kg6.82x higher
Stiffness to weight1.61MN·m/kg25MN·m/kg15.5x higher
Poisson's ratio0.42sourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)0.342sourcewrought TIMETAL 6-4 (TIMET measurement, mean of 10); composition-level, not DMLS-measured
Shear modulus0.511GPa41GPa80.3x stiffer in shear
Bulk modulus3.02GPa116GPa
Speed of sound1,269m/s5,000m/s
Thermal
Thermal conductivity0.17–0.22W/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)6.6W/m·Ksourcebase material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
Thermal expansion80–100µm/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)9µm/m·Ksourcemean 25-100 °C, ASTM E228; EOS Ti64 Grade 23 (=ELI) on EOS M 290 40 µm; condition not stated (sheet's mechanical data are heat treated)
100 mm part over a 50 °C swing450µm growth45µm growth10x less
Specific heatnot sourced580J/kg·Ksourcebase material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
Heats up and cools (diffusivity)not sourced2.59mm²/s
Thermal shock resistance28.6W/m4,825W/m169x more resistant
Melting pointnot sourced1,630–1,650°Csourcemelting range, wrought TIMETAL 6-4 (composition-level)
Max service temperature90°CsourceHDT 0.45 MPa (ISO 75B), unannealednot sourced
Values forLyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO valuesEOS Titanium Ti64ELI (powder 9011-0040; ASTM F136/F3001, i.e. Grade 23) on EOS M400 SF, parameter set Ti64ELI_030_FlexM400_100, 30 µm, as built; ISO 6892-1 A14

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS Ti-6Al-4V ELI Titanium is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic Polypropylene stronger than DMLS Ti-6Al-4V ELI Titanium?

DMLS Ti-6Al-4V ELI Titanium is stronger: its yield strength is 1,100 MPa against 33 MPa for Plastic Polypropylene (33.3x).

Which is lighter, Plastic Polypropylene or DMLS Ti-6Al-4V ELI Titanium?

Plastic Polypropylene is lighter: 900 kg/m³ against 4,400 kg/m³ for DMLS Ti-6Al-4V ELI Titanium.

Which is stiffer, Plastic Polypropylene or DMLS Ti-6Al-4V ELI Titanium?

DMLS Ti-6Al-4V ELI Titanium is stiffer: Young's modulus 110 GPa against 1.45 GPa for Plastic Polypropylene, so the same part in DMLS Ti-6Al-4V ELI Titanium deflects less under the same load.

Which is lighter for the same job, Plastic Polypropylene or DMLS Ti-6Al-4V ELI Titanium?

For the same stiffness or strength: Plastic Polypropylene is lighter for a stiff panel or plate; DMLS Ti-6Al-4V ELI Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PolypropyleneDMLS Ti-6Al-4V ELI Titanium
Stiff rod or tie (tension)15.5x heavierlighter
Stiff beam (bending)1.78x heavierlighter
Stiff panel or platelighter15% heavier
Strong rod or tie6.82x heavierlighter
Strong beam2.12x heavierlighter
Strong panel or plate18% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Polypropylene or DMLS Ti-6Al-4V ELI Titanium?

DMLS Ti-6Al-4V ELI Titanium conducts heat better: 6.6 W/m·K against 0.195 W/m·K for Plastic Polypropylene.

Which expands less with temperature?

DMLS Ti-6Al-4V ELI Titanium expands less: 9 µm/m·K against 90 µm/m·K for Plastic Polypropylene.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PolypropyleneDMLS Ti-6Al-4V ELI Titanium
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PolypropyleneDMLS Ti-6Al-4V ELI Titanium
Strength against density