Materials / Compare
SLA Resin Standard vs. Stainless 304 Compare SLA Resin Standard vs. Stainless 304 strength, stiffness, weight and thermal properties.
Change either side
Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless 304 Stainless 316 Stainless 303 Stainless 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall SLA Resin Standard 3D printed (SLA resin) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless 304 Stainless 316 Stainless 303 Stainless 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall Stainless 304 Wrought Try it on a partA bracket to run stress or thermal on, free in your browser Open in LessCAD Open in LessCAD Mechanical Yield strength not given (tensile used) 241 MPa source typical, annealed, 70 °F (21 °C) Ultimate tensile strength 60 MPa source typical 586 MPa source typical, annealed, 70 °F (21 °C) Flexural strength 105 MPa source typical not sourced Elongation at break 8 % source typical 55 % source typical, annealed, in 2 in. (50.8 mm) Young's modulus (stiffness) 2.75 GPa source typical 193 GPa source typical, in tension Density not sourced 8,030 kg/m³ source typical Strength to weight not sourced 30 kN·m/kg Stiffness to weight not sourced 24 MN·m/kg Poisson's ratio not sourced 0.3 source design value (structural stainless steels) Shear modulus not sourced 74.2 GPa Bulk modulus not sourced 161 GPa Speed of sound not sourced 4,903 m/s Thermal Thermal conductivity not sourced 16.2 W/m·K source at 100 °C Thermal expansion not sourced 16.9 µm/m·K source mean, 0–100 °C 100 mm part over a 50 °C swing not sourced 84.5 µm growth Specific heat not sourced 500 J/kg·K source mean, 0–100 °C Heats up and cools (diffusivity) not sourced 4.03 mm²/s Thermal shock resistance not sourced 838 W/m Melting point not sourced 1,399–1,454 °C source melting range Max service temperature 59 °C source HDT 1.8 MPa 899 °C source continuous, oxidation (scaling) limit in air Values for Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated. Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions Is SLA Resin Standard stronger than Stainless 304? Stainless 304 is stronger: its yield strength is 241 MPa against tensile strength 60 MPa for SLA Resin Standard (4.02x).
Which is stiffer, SLA Resin Standard or Stainless 304? Stainless 304 is stiffer: Young's modulus 193 GPa against 2.75 GPa for SLA Resin Standard, so the same part in Stainless 304 deflects less under the same load.
Among 59 materials 1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Aluminum Steel Iron Titanium Steel AISI 1018 Stainless 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless 303 Stainless 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Stainless 304 Stiffness against density 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Rubber Aluminum Steel Iron Titanium Steel AISI 1018 Stainless 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless 303 Stainless 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick Stainless 304 Strength against density