Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
TIMETAL 6-4 PropertiesTIMETarchived copyTitanium Ti-6Al-4V · Yield strength: typical, plate (>0.187 in), annealed, 0.2% offsetTitanium Ti-6Al-4V · Ultimate tensile strength: typical, plate, annealedTitanium Ti-6Al-4V · Elongation at break: typical, in 2 in., plate annealedTitanium Ti-6Al-4V · Density: nominalTitanium Ti-6Al-4V · Poisson's ratio: mean of TIMET measurementsTitanium Ti-6Al-4V · Melting point: melting rangeTitanium Ti-6Al-4V · Max service temperature: upper recommended use temperature
2
Linatex Premium Rubber Spec Sheet (WMD0118, 2023)Weir MineralsRubber · Ultimate tensile strength: typicalRubber · Elongation at break: typicalRubber · Density: typical (specific gravity)Rubber · Max service temperature: continuous use operating range
3
TIMETAL 6-4 Data SheetTIMETarchived copyTitanium Ti-6Al-4V · Young's modulus (stiffness): typical range, 20 °CTitanium Ti-6Al-4V · Thermal conductivity: typical, 20 °C, mill annealedTitanium Ti-6Al-4V · Thermal expansion: typical, mean 0-100 °CTitanium Ti-6Al-4V · Specific heat: typical, 20 °C
4
Compressibility of Natural Rubber at Pressures Below 500 kg/cm², J. Res. NBS 68A (1964)National Institute of Standards and Technologyarchived copyRubber · Poisson's ratio: government (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation (0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).)Rubber · Specific heat: government (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C
5
Thermal Conductivity of Soft Vulcanized Natural Rubber: Selected Values (AD 643325)Defense Technical Information Centerarchived copyRubber · Thermal conductivity: government selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Rubber stronger than Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V is stronger: its yield strength is 885 MPa against tensile strength 23 MPa for Rubber (38.5x).
Which is lighter, Rubber or Titanium Ti-6Al-4V?
Rubber is lighter: 960 kg/m³ against 4,430 kg/m³ for Titanium Ti-6Al-4V.
Which is lighter for the same job, Rubber or Titanium Ti-6Al-4V?
For the same stiffness or strength: Titanium Ti-6Al-4V is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Rubber
Titanium Ti-6Al-4V
Strong rod or tie
8.34x heavier
lighter
Strong beam
2.47x heavier
lighter
Strong panel or plate
34% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Rubber or Titanium Ti-6Al-4V?
Rubber stretches further before it breaks: 830% elongation at break against 16% for Titanium Ti-6Al-4V.
Thermal
Which handles higher temperatures, Rubber or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V does: 400 °C against 70 °C for Rubber.
Which conducts heat better, Rubber or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V conducts heat better: 6.6 W/m·K against 0.151 W/m·K for Rubber.