Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Synthetic single-crystal silicon (cubic, diamond structure), Korth Kristalle (crystal grower) material data; Korth usually supplies Floating Zone (FZ) material, Czochralski (Cz) also offered. Silicon is elastically anisotropic; the producer quotes one modulus and the solver is isotropic.
SLA Resin Elastic 50A
Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.
1
Si: SiliconKorth Kristallearchived copySilicon · Ultimate tensile strength: modulus of rupture (bending fracture stress); brittle, no yield pointSilicon · Flexural strength: modulus of ruptureSilicon · Young's modulus (stiffness): typical (single quoted value of an anisotropic crystal)Silicon · Density: typicalSilicon · Poisson's ratio: typicalSilicon · Thermal conductivity: typical at 313 K (40 °C)Silicon · Thermal expansion: typical at 300 KSilicon · Specific heat: typicalSilicon · Melting point: typicalSilicon · Max service temperature: producer's maximum application temperature (optical components)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Silicon stronger than SLA Resin Elastic 50A?
Silicon is stronger: its tensile strength is 130 MPa against 3.4 MPa for SLA Resin Elastic 50A (38.2x).
Which is lighter, Silicon or SLA Resin Elastic 50A?
SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 2,329 kg/m³ for Silicon.
Which is lighter for the same job, Silicon or SLA Resin Elastic 50A?
For the same stiffness or strength: Silicon is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Silicon
SLA Resin Elastic 50A
Strong rod or tie
lighter
16.6x heavier
Strong beam
lighter
4.92x heavier
Strong panel or plate
lighter
2.68x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).