Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: American Institute of Steel Construction, Formlabs, bauforumstahl (ArcelorMittal), Ovako
SLA Resin Elastic 50A
Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.
Steel A992
ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
1
Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel A992 · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel A992 · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel A992 · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel A992 · Young's modulus (stiffness): design value (AISC 360-16)Steel A992 · Poisson's ratio: design value (AISC 360-16 Commentary)
4
Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel A992 · Density: nominal (constructional data)Steel A992 · Thermal conductivity: nominal at 20 °CSteel A992 · Thermal expansion: nominal (constructional data, no temperature range stated)
5
S275JR Steel GradeOvakoSteel A992 · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is SLA Resin Elastic 50A stronger than Steel A992?
Steel A992 is stronger: its yield strength is 385 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (113x).
Which is lighter, SLA Resin Elastic 50A or Steel A992?
SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 7,850 kg/m³ for Steel A992.
Which is lighter for the same job, SLA Resin Elastic 50A or Steel A992?
For the same stiffness or strength: Steel A992 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
SLA Resin Elastic 50A
Steel A992
Strong rod or tie
14.6x heavier
lighter
Strong beam
3.01x heavier
lighter
Strong panel or plate
37% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, SLA Resin Elastic 50A or Steel A992?
SLA Resin Elastic 50A stretches further before it breaks: 160% elongation at break against 24.2% for Steel A992.