Materials / Compare

SLA Resin Standard vs. SLA Resin Tough 2000

Compare SLA Resin Standard vs. SLA Resin Tough 2000 strength, stiffness, weight and thermal properties.

Change either side
SLA Resin Standard3D printed (SLA resin)
SLA Resin Tough 20003D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)40.4MPasourcetypical
Ultimate tensile strength60MPasourcetypical49% stronger40.4MPasourcetypical
Flexural strength105MPasourcetypical1.57x stronger in bending67MPasourcetypical
Elongation at break8%sourcetypical79%sourcetypical9.88x more ductile
Young's modulus (stiffness)2.75GPasourcetypical1.53x stiffer1.8GPasourcetypical
Densitynot sourced1,090kg/m³sourcetypical
Strength to weightnot sourced37.1kN·m/kg
Stiffness to weightnot sourced1.65MN·m/kg
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourced1,285m/s
Thermal
Thermal conductivitynot sourcednot sourced
Thermal expansionnot sourced134µm/m·Ksourcemean 0-150 °C
100 mm part over a 50 °C swingnot sourced671µm growth
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistancenot sourcednot sourced
Glass transitionnot sourced112°CsourceDMA
Max service temperature59°CsourceHDT 1.8 MPa57°CsourceHDT 1.8 MPa
Values forFormlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Standard and SLA Resin Tough 2000 are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is SLA Resin Standard stronger than SLA Resin Tough 2000?

SLA Resin Standard is stronger: its tensile strength is 60 MPa against yield strength 40.4 MPa for SLA Resin Tough 2000 (49%).

Which is stiffer, SLA Resin Standard or SLA Resin Tough 2000?

SLA Resin Standard is stiffer: Young's modulus 2.75 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in SLA Resin Standard deflects less under the same load.

Which is more ductile, SLA Resin Standard or SLA Resin Tough 2000?

SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 8% for SLA Resin Standard.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelSLA Resin Tough 2000
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickSLA Resin Tough 2000
Strength against density