Materials / Compare

SLA Resin Tough 2000 vs. Stainless Steel 304

Compare SLA Resin Tough 2000 vs. Stainless Steel 304 strength, stiffness, weight and thermal properties.

SLA Resin Tough 20003D printed (SLA resin)
Stainless Steel 304Wrought
MechanicalSLA Resin Tough 2000Stainless Steel 304
Yield strength40.4MPa1241MPa25.97x stronger
Ultimate tensile strength40.4MPa1586MPa214.5x stronger
Flexural strength67MPa1not sourced
Elongation at break79%144% more ductile55%2
Young's modulus (stiffness)1.8GPa1193GPa2107x stiffer
Density1,090kg/m³17.37x lighter8,030kg/m³2
Strength to weight37.1kN·m/kg23% higher30kN·m/kg
Stiffness to weight1.65MN·m/kg24MN·m/kg14.6x higher
Poisson's rationot sourceddesign value0.33
Shear modulusnot sourced74.2GPa
Bulk modulusnot sourced161GPa
Speed of sound1,285m/s4,903m/s3.82x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30SLA Resin Tough 2000Stainless Steel 304
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30SLA Resin Tough 2000Stainless Steel 304
Strength against densityHigher and further left: stronger for its weight
ThermalSLA Resin Tough 2000Stainless Steel 304
Thermal conductivitynot sourcedat 100 °C16.2W/m·K2
Thermal expansionmean 0-150 °C134µm/m·K1mean16.9µm/m·K27.94x less
100 mm part over a 50 °C swing671µm growth84.5µm growth7.94x less
Specific heatnot sourcedmean500J/kg·K2
Heats up and cools (diffusivity)not sourced4.03mm²/s
Thermal shock resistancenot sourced838W/m
Melting pointnot sourcedmelting range1,399–1,454°C2
Glass transitionDMA112°C1not sourced
Max service temperatureHDT 1.8 MPa57°C1continuous899°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Stainless Steel 304
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Stainless Steel 304
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Formlabs, Cleveland-Cliffs, Steel Construction Institute
SLA Resin Tough 2000
Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.
Stainless Steel 304
Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
  1. 1
    Tough 2000 Resin V2 Technical Data Sheet (2025)Formlabsarchived copySLA Resin Tough 2000 · Yield strength: typicalSLA Resin Tough 2000 · Ultimate tensile strength: typicalSLA Resin Tough 2000 · Flexural strength: typicalSLA Resin Tough 2000 · Elongation at break: typicalSLA Resin Tough 2000 · Young's modulus (stiffness): typicalSLA Resin Tough 2000 · Density: typicalSLA Resin Tough 2000 · Thermal expansion: mean 0-150 °CSLA Resin Tough 2000 · Glass transition: DMASLA Resin Tough 2000 · Max service temperature: HDT 1.8 MPa
  2. 2
    304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
  3. 3
    Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is SLA Resin Tough 2000 stronger than Stainless Steel 304?

Stainless Steel 304 is stronger: its yield strength is 241 MPa against 40.4 MPa for SLA Resin Tough 2000 (5.97x).

Which is lighter, SLA Resin Tough 2000 or Stainless Steel 304?

SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.

Which is stiffer, SLA Resin Tough 2000 or Stainless Steel 304?

Stainless Steel 304 is stiffer: Young's modulus 193 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Stainless Steel 304 deflects less under the same load.

Which is lighter for the same job, SLA Resin Tough 2000 or Stainless Steel 304?

For the same stiffness or strength: SLA Resin Tough 2000 is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 304 is lighter for a stiff rod or tie (tension), stiff beam (bending).

Part that must beSLA Resin Tough 2000Stainless Steel 304
Stiff rod or tie (tension)14.6x heavierlighter
Stiff beam (bending)41% heavierlighter
Stiff panel or platelighter1.55x heavier
Strong rod or tielighter23% heavier
Strong beamlighter2.24x heavier
Strong panel or platelighter3.02x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, SLA Resin Tough 2000 or Stainless Steel 304?

SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 55% for Stainless Steel 304.

Thermal

Which expands less with temperature?

Stainless Steel 304 expands less: 16.9 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.