Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Carpenter Technology, EOS GmbH, U.S. Department of Defense
SLS PA12 Nylon
EOS PA 2200 (PA12) Material Data Sheet, process parameter 'Balance' at 120 µm layer thickness, X orientation, dry (conditioned values not given). Live MDS status 04.10.2026, last changed 10.09.2026; PDF via ?topdf=... link on the same page.
PA 2200 Balance Material Data SheetEOS GmbHSLS PA12 Nylon · Ultimate tensile strength: typicalSLS PA12 Nylon · Elongation at break: typicalSLS PA12 Nylon · Young's modulus (stiffness): typicalSLS PA12 Nylon · Density: typicalSLS PA12 Nylon · Melting point: typicalSLS PA12 Nylon · Max service temperature: HDT 1.8 MPa, X orientation
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 4340 · Young's modulus (stiffness): MIL-HDBK-5J design value (AISI 4340, quenched and tempered)Steel AISI 4340 · Poisson's ratio: MIL-HDBK-5J design value (AISI 4340, quenched and tempered)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLS PA12 Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is SLS PA12 Nylon stronger than Steel AISI 4340?
Steel AISI 4340 is stronger: its yield strength is 1,035 MPa against tensile strength 48 MPa for SLS PA12 Nylon (21.6x).
Which is lighter, SLS PA12 Nylon or Steel AISI 4340?
SLS PA12 Nylon is lighter: 930 kg/m³ against 7,840 kg/m³ for Steel AISI 4340.
Which is stiffer, SLS PA12 Nylon or Steel AISI 4340?
Steel AISI 4340 is stiffer: Young's modulus 200 GPa against 1.65 GPa for SLS PA12 Nylon, so the same part in Steel AISI 4340 deflects less under the same load.
Which is lighter for the same job, SLS PA12 Nylon or Steel AISI 4340?
For the same stiffness or strength: SLS PA12 Nylon is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel AISI 4340 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.
Part that must be
SLS PA12 Nylon
Steel AISI 4340
Stiff rod or tie (tension)
14.4x heavier
lighter
Stiff beam (bending)
31% heavier
lighter
Stiff panel or plate
lighter
1.7x heavier
Strong rod or tie
2.56x heavier
lighter
Strong beam
lighter
9% heavier
Strong panel or plate
lighter
1.82x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).