Solder SAC305 vs. Wood

Compare Solder SAC305 vs. Wood strength, stiffness, weight and thermal properties.

Solder SAC305Cast
WoodNatural
MechanicalSolder SAC305Wood
Yield strength22MPa1not given (tensile used)
Ultimate tensile strength39.6MPa1modulus of rupture99MPa2
Compressive strengthnot sourced46.6MPa2
Flexural strengthnot sourcedmodulus of rupture99MPa2
Elongation at break49%1not sourced
Young's modulus (stiffness)6.9GPa1bending MOE12.5GPa21.81x stiffer
Density7,350kg/m³1681–702kg/m³3
Strength to weight2.99kN·m/kg143kN·m/kg47.8x higher
Stiffness to weight0.939MN·m/kg18.1MN·m/kg19.3x higher
Poisson's ratio0.351mu_LR0.352
Shear modulus2.56GPa4.63GPa1.81x stiffer in shear
Bulk modulus7.67GPa13.9GPa1.81x higher
Speed of sound969m/s4,252m/s4.39x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DPlastic PBT GF30Plastic PPS GF40Plastic LCP GF30Solder SAC305Wood
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DPlastic PBT GF30Plastic PPS GF40Plastic LCP GF30Solder SAC305Wood
Strength against densityHigher and further left: stronger for its weight
ThermalSolder SAC305Wood
Thermal conductivity61W/m·K1339x more heat through a finacross grain0.18W/m·K4
Thermal expansionmean21.9µm/m·K5parallel to grain3.1–4.5µm/m·K4
100 mm part over a 50 °C swing110µm growth19µm growth5.76x less
Specific heat232J/kg·K5solid wood1,700J/kg·K47.33x higher
Heats up and cools (diffusivity)35.8mm²/s234x faster0.153mm²/s
Thermal shock resistance5,773W/m23.7x more resistant244W/m
Melting pointsolidus-liquidus217–220°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DPlastic PBT GF30Plastic PPS GF40Plastic LCP GF30Solder SAC305Wood
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DPlastic PBT GF30Plastic PPS GF40Plastic LCP GF30Solder SAC305Wood
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Indium Corporation, USDA Forest Products Laboratory, MacDermid Alpha
Solder SAC305
SAC305 (Sn96.5Ag3.0Cu0.5) solder alloy, bulk; Indium Corporation Indalloy 256 (SAC305) for Preforms product data sheet (Form No. 100346 R0, 2024), selected properties, test temperature not stated; expansion and specific heat from MacDermid Alpha VACULOY SAC TDS (06 September 2023).
Wood
Northern red oak (Quercus rubra), clear straight-grained specimens at 12% MC, parallel to grain unless stated; USDA FPL Wood Handbook FPL-GTR-282 (2021) Ch. 4 and Ch. 5
  1. 1
    Indalloy 256 (SAC305) for Preforms Product Data Sheet (100346 R0)Indium Corporationarchived copySolder SAC305 · Yield strength: typicalSolder SAC305 · Ultimate tensile strength: typicalSolder SAC305 · Elongation at break: typicalSolder SAC305 · Young's modulus (stiffness): typical, temperature and strain rate not statedSolder SAC305 · Density: typicalSolder SAC305 · Poisson's ratio: typicalSolder SAC305 · Thermal conductivity: typical, temperature not statedSolder SAC305 · Melting point: solidus-liquidus
  2. 2
    Wood Handbook (FPL-GTR-282), Chapter 5: Mechanical Properties of WoodUSDA Forest Products LaboratoryWood · Ultimate tensile strength: modulus of rupture (no direct tensile value)Wood · Compressive strength: compression parallel to grain (maximum crushing strength), 12% MCWood · Flexural strength: modulus of rupture (static bending), 12% MCWood · Young's modulus (stiffness): bending MOE, parallel to grainWood · Poisson's ratio: mu_LR (red oak group, ~12% MC)
  3. 3
    Technical Note 218: Weights of Various Woods Grown in the United States (1953)USDA Forest Products LaboratoryWood · Density: average weight of clear wood at 8% and 15% moisture content
  4. 4
    Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of WoodUSDA Forest Products LaboratoryWood · Thermal conductivity: across grain, 12% MC (Table 4-7, approximate)Wood · Thermal expansion: parallel to grain, ovendry wood, range across speciesWood · Specific heat: solid wood (all species), 12% MC, 27 C
  5. 5
    ALPHA Vaculoy SAC Alloys Technical Data Sheet (2023)MacDermid AlphaSolder SAC305 · Thermal expansion: mean, 20-100 °C (MacDermid Alpha)Solder SAC305 · Specific heat: typical (MacDermid Alpha)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Solder SAC305 stronger than Wood?

Wood is stronger: its tensile strength is 99 MPa against yield strength 22 MPa for Solder SAC305 (4.5x).

Which is lighter, Solder SAC305 or Wood?

Wood is lighter: 692 kg/m³ against 7,350 kg/m³ for Solder SAC305.

Which is stiffer, Solder SAC305 or Wood?

Wood is stiffer: Young's modulus 12.5 GPa against 6.9 GPa for Solder SAC305, so the same part in Wood deflects less under the same load.

Which is lighter for the same job, Solder SAC305 or Wood?

For the same stiffness or strength: Wood is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beSolder SAC305Wood
Stiff rod or tie (tension)19.3x heavierlighter
Stiff beam (bending)14.3x heavierlighter
Stiff panel or plate13x heavierlighter
Strong rod or tie47.8x heavierlighter
Strong beam29x heavierlighter
Strong panel or plate22.5x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Solder SAC305 or Wood?

Solder SAC305 conducts heat better: 61 W/m·K against 0.18 W/m·K for Wood.

Which expands less with temperature?

Wood expands less: 3.8 µm/m·K against 21.9 µm/m·K for Solder SAC305.