Materials / Compare
Concrete vs. Solder SAC305 Compare Concrete vs. Solder SAC305 strength, stiffness, weight and thermal properties.
Change either side
Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Concrete Cast Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Solder SAC305 Cast Try it on a partA sample part to run stress or thermal on, free in your browser Open in LessCAD Open in LessCAD Mechanical Yield strength not sourced 22 MPa source typical Ultimate tensile strength not sourced 39.6 MPa source typical Compressive strength 27.6 MPa source specified compressive strength class (f'c), not a measured typical not sourced Elongation at break not sourced 49 % source typical Young's modulus (stiffness) not sourced 6.9 GPa source typical, temperature and strain rate not stated Density 2,240–2,400 kg/m³ source range for normalweight concrete 7,350 kg/m³ source typical Strength to weight not sourced 2.99 kN·m/kg Stiffness to weight not sourced 0.939 MN·m/kg Poisson's ratio 0.15–0.2 source general range at normal ambient conditions (overall 0.11-0.32) 0.35 source typical Shear modulus not sourced 2.56 GPa Bulk modulus not sourced 7.67 GPa Speed of sound not sourced 969 m/s Thermal Thermal conductivity 0.9 W/m·K source typical (comparative value) 61 W/m·K source typical, temperature not stated Thermal expansion 8–12 µm/m·K source typical range for portland cement concrete (aggregate dependent) 21.9 µm/m·K source mean, 20-100 °C (MacDermid Alpha) 100 mm part over a 50 °C swing 50 µm growth 2.19x less 110 µm growth Specific heat 900 J/kg·K source typical (NIST guidance for thermal analysis) 232 J/kg·K source typical (MacDermid Alpha) Heats up and cools (diffusivity) 0.431 mm²/s 35.8 mm²/s 83x faster Thermal shock resistance not sourced 5,773 W/m Melting point not sourced 217–220 °C source solidus-liquidus Max service temperature 65 °C source code long-term temperature limit (ASME Code, concrete containments) not sourced Values for Normal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC review SAC305 (Sn96.5Ag3.0Cu0.5) solder alloy, bulk; Indium Corporation Indalloy 256 (SAC305) for Preforms product data sheet (Form No. 100346 R0, 2024), selected properties, test temperature not stated; expansion and specific heat from MacDermid Alpha VACULOY SAC TDS (06 September 2023).
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions Which is lighter, Concrete or Solder SAC305? Concrete is lighter: 2,320 kg/m³ against 7,350 kg/m³ for Solder SAC305.
Which conducts heat better, Concrete or Solder SAC305? Solder SAC305 conducts heat better: 61 W/m·K against 0.9 W/m·K for Concrete.
Which expands less with temperature? Concrete expands less: 10 µm/m·K against 21.9 µm/m·K for Solder SAC305.
Among 72 materials 1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum ADC12 Magnesium AZ91D Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Solder SAC305 Stiffness against density 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Rubber Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick PCB Laminate FR-4 Silicon Ceramic Alumina 96% Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum ADC12 Magnesium AZ91D Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Solder SAC305 Strength against density