Materials / Compare

Stainless Steel 304 vs. Steel A992

Compare Stainless Steel 304 vs. Steel A992 strength, stiffness, weight and thermal properties.

Change either side
Stainless Steel 304Wrought
Steel A992Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength241MPasourcetypical, annealed, 70 °F (21 °C)385MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISC
Ultimate tensile strength586MPasourcetypical, annealed, 70 °F (21 °C)505MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)
Elongation at break55%sourcetypical, annealed, in 2 in. (50.8 mm)not sourced
Young's modulus (stiffness)193GPasourcetypical, in tension200GPasourcedesign value (AISC 360-16)
Density8,030kg/m³sourcetypical7,850kg/m³sourcenominal (constructional data)
Strength to weight30kN·m/kg49kN·m/kg1.63x higher
Stiffness to weight24MN·m/kg25.5MN·m/kg6% higher
Poisson's ratio0.3sourcedesign value (structural stainless steels)0.3sourcedesign value (AISC 360-16 Commentary)
Shear modulus74.2GPa76.9GPa4% stiffer in shear
Bulk modulus161GPa167GPa
Speed of sound4,903m/s5,048m/s
Thermal
Thermal conductivity16.2W/m·Ksourceat 100 °C48W/m·Ksourcenominal at 20 °C
Thermal expansion16.9µm/m·Ksourcemean, 0–100 °C12µm/m·Ksourcenominal (constructional data, no temperature range stated)
100 mm part over a 50 °C swing84.5µm growth60µm growth41% less
Specific heat500J/kg·Ksourcemean, 0–100 °C460–480J/kg·Ksourcebase material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Heats up and cools (diffusivity)4.03mm²/s13mm²/s3.22x faster
Thermal shock resistance838W/m5,390W/m6.43x more resistant
Melting point1,399–1,454°Csourcemelting rangenot sourced
Max service temperature899°Csourcecontinuous, oxidation (scaling) limit in airnot sourced
Values forType 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manualASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Stainless Steel 304 stronger than Steel A992?

Steel A992 is stronger: its yield strength is 385 MPa against 241 MPa for Stainless Steel 304 (1.6x).

Which is lighter, Stainless Steel 304 or Steel A992?

Steel A992 is lighter: 7,850 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.

Which is stiffer, Stainless Steel 304 or Steel A992?

Steel A992 is stiffer: Young's modulus 200 GPa against 193 GPa for Stainless Steel 304, so the same part in Steel A992 deflects less under the same load.

Which is lighter for the same job, Stainless Steel 304 or Steel A992?

For the same stiffness or strength: Steel A992 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beStainless Steel 304Steel A992
Stiff rod or tie (tension)6% heavierlighter
Stiff beam (bending)4% heavierlighter
Stiff panel or plate4% heavierlighter
Strong rod or tie1.63x heavierlighter
Strong beam40% heavierlighter
Strong panel or plate29% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Stainless Steel 304 or Steel A992?

Steel A992 conducts heat better: 48 W/m·K against 16.2 W/m·K for Stainless Steel 304.

Which expands less with temperature?

Steel A992 expands less: 12 µm/m·K against 16.9 µm/m·K for Stainless Steel 304.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Stainless Steel 304Steel A992
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Stainless Steel 304Steel A992
Strength against density

Related comparisons