Materials / Compare

Steel A992 vs. DMLS Ti-6Al-4V ELI Titanium

Compare Steel A992 vs. DMLS Ti-6Al-4V ELI Titanium strength, stiffness, weight and thermal properties.

Change either side
Steel A992Wrought
DMLS Ti-6Al-4V ELI Titanium3D printed metal (DMLS)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength385MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISC1,100MPasourcetypical, as built, average of horizontal + vertical (M400)
Ultimate tensile strength505MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)1,270MPasourcetypical, as built, average of horizontal + vertical (M400)
Elongation at breaknot sourced8.7%sourcetypical at break, as built (M400)
Young's modulus (stiffness)200GPasourcedesign value (AISC 360-16)110GPasourcesame maker and process, sibling grade: EOS Titanium Ti64 (Grade 5) on EOS M 290, as built, XY and Z, typical
Density7,850kg/m³sourcenominal (constructional data)4,400kg/m³sourcetypical part density (ISO 3369), M400
Strength to weight49kN·m/kg250kN·m/kg5.1x higher
Stiffness to weight25.5MN·m/kg2% higher25MN·m/kg
Poisson's ratio0.3sourcedesign value (AISC 360-16 Commentary)0.342sourcewrought TIMETAL 6-4 (TIMET measurement, mean of 10); composition-level, not DMLS-measured
Shear modulus76.9GPa1.88x stiffer in shear41GPa
Bulk modulus167GPa116GPa
Speed of sound5,048m/s5,000m/s
Thermal
Thermal conductivity48W/m·Ksourcenominal at 20 °C6.6W/m·Ksourcebase material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
Thermal expansion12µm/m·Ksourcenominal (constructional data, no temperature range stated)9µm/m·Ksourcemean 25-100 °C, ASTM E228; EOS Ti64 Grade 23 (=ELI) on EOS M 290 40 µm; condition not stated (sheet's mechanical data are heat treated)
100 mm part over a 50 °C swing60µm growth45µm growth33% less
Specific heat460–480J/kg·Ksourcebase material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C580J/kg·Ksourcebase material: wrought Ti-6Al-4V / 6-4 ELI (TIMET datasheet), 20 °C
Heats up and cools (diffusivity)13mm²/s5.03x faster2.59mm²/s
Thermal shock resistance5,390W/m12% more resistant4,825W/m
Melting pointnot sourced1,630–1,650°Csourcemelting range, wrought TIMETAL 6-4 (composition-level)
Values forASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.EOS Titanium Ti64ELI (powder 9011-0040; ASTM F136/F3001, i.e. Grade 23) on EOS M400 SF, parameter set Ti64ELI_030_FlexM400_100, 30 µm, as built; ISO 6892-1 A14

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS Ti-6Al-4V ELI Titanium is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Steel A992 stronger than DMLS Ti-6Al-4V ELI Titanium?

DMLS Ti-6Al-4V ELI Titanium is stronger: its yield strength is 1,100 MPa against 385 MPa for Steel A992 (2.86x).

Which is lighter, Steel A992 or DMLS Ti-6Al-4V ELI Titanium?

DMLS Ti-6Al-4V ELI Titanium is lighter: 4,400 kg/m³ against 7,850 kg/m³ for Steel A992.

Which is stiffer, Steel A992 or DMLS Ti-6Al-4V ELI Titanium?

Steel A992 is stiffer: Young's modulus 200 GPa against 110 GPa for DMLS Ti-6Al-4V ELI Titanium, so the same part in Steel A992 deflects less under the same load.

Which is lighter for the same job, Steel A992 or DMLS Ti-6Al-4V ELI Titanium?

For the same stiffness or strength: Steel A992 is lighter for a stiff rod or tie (tension); DMLS Ti-6Al-4V ELI Titanium is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beSteel A992DMLS Ti-6Al-4V ELI Titanium
Stiff rod or tie (tension)lighter2% heavier
Stiff beam (bending)32% heavierlighter
Stiff panel or plate46% heavierlighter
Strong rod or tie5.1x heavierlighter
Strong beam3.59x heavierlighter
Strong panel or plate3.02x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Steel A992 or DMLS Ti-6Al-4V ELI Titanium?

Steel A992 conducts heat better: 48 W/m·K against 6.6 W/m·K for DMLS Ti-6Al-4V ELI Titanium.

Which expands less with temperature?

DMLS Ti-6Al-4V ELI Titanium expands less: 9 µm/m·K against 12 µm/m·K for Steel A992.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelSteel A992DMLS Ti-6Al-4V ELI Titanium
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickSteel A992DMLS Ti-6Al-4V ELI Titanium
Strength against density