Materials / Compare
Aluminum 7075-T6 vs. Plastic Polypropylene
Compare Aluminum 7075-T6 vs. Plastic Polypropylene strength, stiffness, weight and thermal properties.
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|---|---|
| Mechanical | ||
| Yield strength | 503MPasourcetypical, 0.2% offset, .500 in dia specimen | 33MPasourcetypical, tensile stress at yield ISO 527 |
| Ultimate tensile strength | 572MPasourcetypical | not sourced |
| Elongation at break | 11%sourcetypical, in 4D | not sourced |
| Young's modulus (stiffness) | 71GPasourcetypical | 1.45GPasourcetypical, tensile modulus ISO 527 |
| Density | 2,800kg/m³sourcenominal | 900kg/m³sourcetypical, 23 °C ISO 1183-1 |
| Strength to weight | 180kN·m/kg4.9x higher | 36.7kN·m/kg |
| Stiffness to weight | 25.4MN·m/kg15.7x higher | 1.61MN·m/kg |
| Poisson's ratio | 0.33sourcetypical (handbook physical constant) | 0.42sourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene) |
| Shear modulus | 26.7GPa52.3x stiffer in shear | 0.511GPa |
| Bulk modulus | 69.6GPa | 3.02GPa |
| Speed of sound | 5,036m/s | 1,269m/s |
| Thermal | ||
| Thermal conductivity | 130W/m·Ksourcetypical, 20 °C, T651 | 0.17–0.22W/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene) |
| Thermal expansion | 23.4µm/m·Ksourcetypical, mean 20-100 °C | 80–100µm/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene) |
| 100 mm part over a 50 °C swing | 117µm growth3.85x less | 450µm growth |
| Specific heat | 960J/kg·Ksourcetypical, at 100 °C | not sourced |
| Heats up and cools (diffusivity) | 48.4mm²/s | not sourced |
| Thermal shock resistance | 26,370W/m922x more resistant | 28.6W/m |
| Melting point | 532–635°Csourcemelting range | not sourced |
| Max service temperature | not sourced | 90°CsourceHDT 0.45 MPa (ISO 75B), unannealed |
| Values for | 7075-T6/T651, Kaiser Aluminum rod & bar (mechanical) and sheet/coil/plate (physical) typical datasheets; Poisson from MIL-HDBK-5J | LyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO values |
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Is Aluminum 7075-T6 stronger than Plastic Polypropylene?
Aluminum 7075-T6 is stronger: its yield strength is 503 MPa against 33 MPa for Plastic Polypropylene (15.2x).
Which is lighter, Aluminum 7075-T6 or Plastic Polypropylene?
Plastic Polypropylene is lighter: 900 kg/m³ against 2,800 kg/m³ for Aluminum 7075-T6.
Which is stiffer, Aluminum 7075-T6 or Plastic Polypropylene?
Aluminum 7075-T6 is stiffer: Young's modulus 71 GPa against 1.45 GPa for Plastic Polypropylene, so the same part in Aluminum 7075-T6 deflects less under the same load.
Which is lighter for the same job, Aluminum 7075-T6 or Plastic Polypropylene?
For the same stiffness or strength: Aluminum 7075-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
| Part that must be | Aluminum 7075-T6 | Plastic Polypropylene |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 15.7x heavier |
| Stiff beam (bending) | lighter | 2.25x heavier |
| Stiff panel or plate | lighter | 18% heavier |
| Strong rod or tie | lighter | 4.9x heavier |
| Strong beam | lighter | 1.98x heavier |
| Strong panel or plate | lighter | 25% heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which conducts heat better, Aluminum 7075-T6 or Plastic Polypropylene?
Aluminum 7075-T6 conducts heat better: 130 W/m·K against 0.195 W/m·K for Plastic Polypropylene.
Which expands less with temperature?
Aluminum 7075-T6 expands less: 23.4 µm/m·K against 90 µm/m·K for Plastic Polypropylene.