Materials / Compare

Aluminum 1100-O vs. SLA Resin Elastic 50A

Compare Aluminum 1100-O vs. SLA Resin Elastic 50A strength, stiffness, weight and thermal properties.

Aluminum 1100-OWrought
SLA Resin Elastic 50A3D printed (SLA resin)
MechanicalAluminum 1100-OSLA Resin Elastic 50A
Yield strength35MPa1not given (tensile used)
Ultimate tensile strength90MPa126.5x stronger3.4MPa2
Elongation at break35%1160%24.57x more ductile
Young's modulus (stiffness)69GPa1not sourced
Density2,710kg/m³11,010kg/m³22.68x lighter
Strength to weight12.9kN·m/kg3.84x higher3.37kN·m/kg
Stiffness to weight25.5MN·m/kgnot sourced
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound5,046m/snot sourced
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-O
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-OSLA Resin Elastic 50A
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 1100-OSLA Resin Elastic 50A
Thermal conductivity222W/m·K1not sourced
Thermal expansion23.6µm/m·K1not sourced
100 mm part over a 50 °C swing118µm growthnot sourced
Specific heatbase material901J/kg·K3not sourced
Heats up and cools (diffusivity)90.9mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Melting pointmelting range640–655°C1not sourced
Glass transitionnot sourcedDMA-34.5°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-O
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-O
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Kaiser Aluminum, Formlabs, Hydro
Aluminum 1100-O
1100-O (annealed) commercially pure aluminium, Kaiser Aluminum Tube & Pipe Alloy 1100 Technical Data (Rev. 05/06), typical properties; specific heat from Hydro EN AW-1050A (99.5% Al) extruded-products datasheet (10/2018).
SLA Resin Elastic 50A
Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.
  1. 1
    Alloy 1100 Tube & Pipe Technical Data, Rev. 05/06Kaiser Aluminumarchived copyAluminum 1100-O · Yield strength: typical, O, 0.0625 in specimenAluminum 1100-O · Ultimate tensile strength: typical, OAluminum 1100-O · Elongation at break: typical, O, in 4DAluminum 1100-O · Young's modulus (stiffness): typicalAluminum 1100-O · Density: nominal, 20 °CAluminum 1100-O · Thermal conductivity: typical, O, 20 °CAluminum 1100-O · Thermal expansion: typical, mean 20-100 °CAluminum 1100-O · Melting point: melting range
  2. 2
    Elastic 50A Resin V2 Technical Data Sheet (2024)Formlabsarchived copySLA Resin Elastic 50A · Ultimate tensile strength: typicalSLA Resin Elastic 50A · Elongation at break: typicalSLA Resin Elastic 50A · Density: typicalSLA Resin Elastic 50A · Glass transition: DMA
  3. 3
    Technical Datasheet, Extruded Products: Alloy EN AW-1050AHydroAluminum 1100-O · Specific heat: base material: commercially pure aluminium EN AW-1050A (Hydro), 20 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Aluminum 1100-O stronger than SLA Resin Elastic 50A?

Aluminum 1100-O is stronger: its yield strength is 35 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (10.3x).

Which is lighter, Aluminum 1100-O or SLA Resin Elastic 50A?

SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 2,710 kg/m³ for Aluminum 1100-O.

Which is lighter for the same job, Aluminum 1100-O or SLA Resin Elastic 50A?

For the same stiffness or strength: Aluminum 1100-O is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 1100-OSLA Resin Elastic 50A
Strong rod or tielighter3.84x heavier
Strong beamlighter1.76x heavier
Strong panel or platelighter20% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 1100-O or SLA Resin Elastic 50A?

SLA Resin Elastic 50A stretches further before it breaks: 160% elongation at break against 35% for Aluminum 1100-O.

Related comparisons