Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: Kaiser Aluminum, Celanese, U.S. Department of Defense
Aluminum 2024-T351
2024-T4/T351, Kaiser Aluminum sheet, coil & plate typical datasheet; Poisson from MIL-HDBK-5J
Plastic UHMWPE
Celanese GUR 4120 (avg. molecular weight 4.7x10^6 g/mol), typical values on compression-molded specimens; CTE and thermal conductivity from Celanese's generic UHMWPE guide (grade not named)
1
Alloy 2024 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 2024-T351 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 2024-T351 · Ultimate tensile strength: typicalAluminum 2024-T351 · Elongation at break: typical, in 4DAluminum 2024-T351 · Young's modulus (stiffness): typicalAluminum 2024-T351 · Density: nominalAluminum 2024-T351 · Thermal conductivity: typical, 20 °CAluminum 2024-T351 · Thermal expansion: typical, mean 20-100 °CAluminum 2024-T351 · Specific heat: typical, at 100 °CAluminum 2024-T351 · Melting point: melting range
2
GUR UHMW-PE Overview (GUR-015)CelanesePlastic UHMWPE · Yield strength: typical, tensile stress at yield ISO 527, 50 mm/minPlastic UHMWPE · Ultimate tensile strength: typical, tensile stress at break ISO 527, 50 mm/minPlastic UHMWPE · Elongation at break: typical, nominal elongation at break ISO 527Plastic UHMWPE · Young's modulus (stiffness): typical, tensile modulus ISO 527, 1 mm/minPlastic UHMWPE · Density: typicalPlastic UHMWPE · Melting point: DSC 10 K/minPlastic UHMWPE · Max service temperature: recommended max constant operating temperature
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 2024-T351 · Poisson's ratio: typical (handbook physical constant), all tempers
4
GUR UHMW-PE Polymer Guide (GUR-003)Celanesearchived copyPlastic UHMWPE · Thermal conductivity: typical, unfilled (narrative value, generic Celanese UHMWPE)Plastic UHMWPE · Thermal expansion: typical, 20 to 100 °C (generic Celanese UHMWPE)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 2024-T351 stronger than Plastic UHMWPE?
Aluminum 2024-T351 is stronger: its yield strength is 324 MPa against 20 MPa for Plastic UHMWPE (16.2x).
Which is lighter, Aluminum 2024-T351 or Plastic UHMWPE?
Plastic UHMWPE is lighter: 930 kg/m³ against 2,770 kg/m³ for Aluminum 2024-T351.
Which is stiffer, Aluminum 2024-T351 or Plastic UHMWPE?
Aluminum 2024-T351 is stiffer: Young's modulus 73.1 GPa against 0.66 GPa for Plastic UHMWPE, so the same part in Aluminum 2024-T351 deflects less under the same load.
Which is lighter for the same job, Aluminum 2024-T351 or Plastic UHMWPE?
For the same stiffness or strength: Aluminum 2024-T351 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 2024-T351
Plastic UHMWPE
Stiff rod or tie (tension)
lighter
37.2x heavier
Stiff beam (bending)
lighter
3.53x heavier
Stiff panel or plate
lighter
1.61x heavier
Strong rod or tie
lighter
5.44x heavier
Strong beam
lighter
2.15x heavier
Strong panel or plate
lighter
35% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 2024-T351 or Plastic UHMWPE?
Plastic UHMWPE stretches further before it breaks: 465% elongation at break against 19% for Aluminum 2024-T351.
Thermal
Which conducts heat better, Aluminum 2024-T351 or Plastic UHMWPE?
Aluminum 2024-T351 conducts heat better: 120 W/m·K against 0.4 W/m·K for Plastic UHMWPE.
Which expands less with temperature?
Aluminum 2024-T351 expands less: 22.9 µm/m·K against 200 µm/m·K for Plastic UHMWPE.