Materials / Compare
Aluminum 5052-H32 vs. FDM Polycarbonate
Compare Aluminum 5052-H32 vs. FDM Polycarbonate strength, stiffness, weight and thermal properties.
| Mechanical | Aluminum 5052-H32 | FDM Polycarbonate |
|---|---|---|
| Yield strength | 195MPa13.66x stronger | 53.3MPa2 |
| Ultimate tensile strength | 230MPa14.32x stronger | 53.3MPa2 |
| Flexural strength | not sourced | 89.4MPa2 |
| Elongation at break | 12%130% more ductile | 9.2%2 |
| Young's modulus (stiffness) | 70GPa129.2x stiffer | 2.39GPa2 |
| Density | 2,685kg/m³3 | range1,180–1,200kg/m³2 |
| Strength to weight | 72.6kN·m/kg1.62x higher | 44.8kN·m/kg |
| Stiffness to weight | 26.1MN·m/kg13x higher | 2.01MN·m/kg |
| Poisson's ratio | 0.333 | base material0.384 |
| Shear modulus | 26.3GPa30.3x stiffer in shear | 0.867GPa |
| Bulk modulus | 68.6GPa20.6x higher | 3.33GPa |
| Speed of sound | 5,106m/s3.6x faster | 1,418m/s |
| Thermal | Aluminum 5052-H32 | FDM Polycarbonate |
|---|---|---|
| Thermal conductivity | base material138W/m·K1690x more heat through a fin | base material0.2W/m·K5 |
| Thermal expansion | 23.8µm/m·K12.73x less | base material65µm/m·K5 |
| 100 mm part over a 50 °C swing | 119µm growth2.73x less | 325µm growth |
| Specific heat | at 100 °C963J/kg·K3 | not sourced |
| Heats up and cools (diffusivity) | 53.4mm²/s | not sourced |
| Thermal shock resistance | 10,822W/m255x more resistant | 42.5W/m |
| Melting point | melting range605–650°C1 | not sourced |
| Glass transition | not sourced | 108°C2 |
| Max service temperature | not sourced | HDT 0.455 MPa105°C2 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources5 documents: Kaiser Aluminum, UltiMaker, U.S. Department of Defense, Covestro
- Aluminum 5052-H32
- 5052-H32, Kaiser Aluminum tube & pipe typical datasheet (mechanical, CTE, melting); MIL-HDBK-5J (Poisson, density, specific heat)
- FDM Polycarbonate
- Ultimaker PC, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 20, 2022.
- 1Alloy 5052 Tube & Pipe Technical DataKaiser Aluminumarchived copyAluminum 5052-H32 · Yield strength: typical, 0.2% offsetAluminum 5052-H32 · Ultimate tensile strength: typicalAluminum 5052-H32 · Elongation at break: typicalAluminum 5052-H32 · Young's modulus (stiffness): typicalAluminum 5052-H32 · Thermal conductivity: base material: 5052 in O temper (same alloy, annealed); Kaiser typicalAluminum 5052-H32 · Thermal expansion: typical, mean 20-100 °CAluminum 5052-H32 · Melting point: melting range
- 2Ultimaker PC Technical Data Sheet, v5.00UltiMakerarchived copyFDM Polycarbonate · Yield strength: typicalFDM Polycarbonate · Ultimate tensile strength: typical, peak stress (= stress at yield)FDM Polycarbonate · Flexural strength: typicalFDM Polycarbonate · Elongation at break: typicalFDM Polycarbonate · Young's modulus (stiffness): typicalFDM Polycarbonate · Density: rangeFDM Polycarbonate · Glass transition: typicalFDM Polycarbonate · Max service temperature: HDT 0.455 MPa (printed specimens)
- 3MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 5052-H32 · Density: nominalAluminum 5052-H32 · Poisson's ratio: typical (handbook physical constant)Aluminum 5052-H32 · Specific heat: at 100 °C (212 °F); table covers O, H32, H34, H36, H38
- 4Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyFDM Polycarbonate · Poisson's ratio: base material: polycarbonate family typical (Covestro Part and Mold Design guide, Table 3-1)
- 5Makrolon 2405 Technical Data SheetCovestroFDM Polycarbonate · Thermal conductivity: base material: Covestro Makrolon 2405 injection-molding PC, typical, through-plane, 23 °CFDM Polycarbonate · Thermal expansion: base material: Covestro Makrolon 2405 injection-molding PC, typical, 23-55 °C, parallel
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM Polycarbonate is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 5052-H32 stronger than FDM Polycarbonate?
Aluminum 5052-H32 is stronger: its yield strength is 195 MPa against 53.3 MPa for FDM Polycarbonate (3.66x).
Which is lighter, Aluminum 5052-H32 or FDM Polycarbonate?
FDM Polycarbonate is lighter: 1,190 kg/m³ against 2,685 kg/m³ for Aluminum 5052-H32.
Which is stiffer, Aluminum 5052-H32 or FDM Polycarbonate?
Aluminum 5052-H32 is stiffer: Young's modulus 70 GPa against 2.39 GPa for FDM Polycarbonate, so the same part in Aluminum 5052-H32 deflects less under the same load.
Which is lighter for the same job, Aluminum 5052-H32 or FDM Polycarbonate?
For the same stiffness or strength: Aluminum 5052-H32 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam; FDM Polycarbonate is lighter for a strong panel or plate.
| Part that must be | Aluminum 5052-H32 | FDM Polycarbonate |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 13x heavier |
| Stiff beam (bending) | lighter | 2.4x heavier |
| Stiff panel or plate | lighter | 37% heavier |
| Strong rod or tie | lighter | 1.62x heavier |
| Strong beam | lighter | 5% heavier |
| Strong panel or plate | 18% heavier | lighter |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 5052-H32 or FDM Polycarbonate?
Aluminum 5052-H32 stretches further before it breaks: 12% elongation at break against 9.2% for FDM Polycarbonate.
Thermal
Which conducts heat better, Aluminum 5052-H32 or FDM Polycarbonate?
Aluminum 5052-H32 conducts heat better: 138 W/m·K against 0.2 W/m·K for FDM Polycarbonate.
Which expands less with temperature?
Aluminum 5052-H32 expands less: 23.8 µm/m·K against 65 µm/m·K for FDM Polycarbonate.
Related comparisons
- Aluminum 5052-H32 vs. Aluminum 6063-T6
- Aluminum 5052-H32 vs. Aluminum A380
- Aluminum 5052-H32 vs. Aluminum ADC12
- Aluminum 5052-H32 vs. DMLS AlSi10Mg Aluminum
- FDM Polycarbonate vs. Plastic Nylon
- FDM Polycarbonate vs. SLA Resin Standard
- FDM Polycarbonate vs. Plastic Polycarbonate
- FDM Polycarbonate vs. Plastic ABS (bulk/injection)