Materials / Compare

Aluminum 6061-T6 vs. Brick

Compare Aluminum 6061-T6 vs. Brick strength, stiffness, weight and thermal properties.

Aluminum 6061-T6Wrought
BrickNatural
MechanicalAluminum 6061-T6Brick
Yield strength276MPa1none (brittle)
Ultimate tensile strength310MPa1modulus of rupture5.1MPa2
Compressive strengthnot sourced77.9MPa3
Elongation at break17%1none (brittle)
Young's modulus (stiffness)68.3GPa1not sourced
Density2,700kg/m³12,082kg/m³430% lighter
Strength to weight102kN·m/kg41.7x higher2.45kN·m/kg
Stiffness to weight25.3MN·m/kgnot sourced
Poisson's ratio0.335not sourced
Shear modulus25.7GPanot sourced
Bulk modulus67GPanot sourced
Speed of sound5,030m/snot sourced
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6061-T6
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6061-T6Brick
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 6061-T6Brick
Thermal conductivity167W/m·K10.92–1.12W/m·K4
Thermal expansion23.6µm/m·K17.2µm/m·K33.28x less
100 mm part over a 50 °C swing118µm growth36µm growth3.28x less
Specific heat896J/kg·K1837J/kg·K6
Heats up and cools (diffusivity)69mm²/s118x faster0.585mm²/s
Thermal shock resistance19,159W/mnot sourced
Melting pointsolidus-liquidus582–652°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6061-T6Brick
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 6061-T6Brick
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources6 documents: Kaiser Aluminum, National Institute of Standards and Technology, Brick Industry Association, U.S. Department of Defense
Aluminum 6061-T6
6061-T6/T651, Kaiser Aluminum typical properties; Poisson from MIL-HDBK-5J
Brick
Solid extruded clay/shale brick units (BIA 1993 manufacturer survey, TN 3A 2024); face brick of 130 lb/ft3 for thermal properties (BIA TN 4, from ASHRAE 2013); CTE is the TMS Code value for clay/shale masonry
  1. 1
    Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 6061-T6 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 6061-T6 · Ultimate tensile strength: typicalAluminum 6061-T6 · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum 6061-T6 · Young's modulus (stiffness): typicalAluminum 6061-T6 · Density: nominalAluminum 6061-T6 · Thermal conductivity: typical, 20 °CAluminum 6061-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 6061-T6 · Specific heat: typical, at 100 °CAluminum 6061-T6 · Melting point: solidus-liquidus
  2. 2
    Strength of Masonry Walls Under Compressive and Transverse Loads (Building Science Series 34)National Institute of Standards and Technologyarchived copyBrick · Ultimate tensile strength: modulus of rupture (no direct tensile value)
  3. 3
    Technical Notes 3A: Brick Masonry Material PropertiesBrick Industry AssociationBrick · Compressive strength: mean unit compressive strength, solid extruded brick (survey mean; SD 30.8 MPa)Brick · Thermal expansion: TMS Code average coefficient, clay/shale unit masonry
  4. 4
    Technical Notes 4: Introduction to Energy Performance of Brick Masonry (2016)Brick Industry Associationarchived copyBrick · Density: face brick density row used for k (BIA notes most fired clay brick 120-130 lb/ft3)Brick · Thermal conductivity: range for 130 lb/ft3 face brick (ASHRAE 2013 via BIA)
  5. 5
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 6061-T6 · Poisson's ratio: typical (handbook physical constant)
  6. 6
    Technical Notes 4B: Energy Code Compliance of Brick Masonry WallsBrick Industry Associationarchived copyBrick · Specific heat: value used in BIA heat-capacity sample calculation

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 6061-T6 stronger than Brick?

Aluminum 6061-T6 is stronger: its yield strength is 276 MPa against tensile strength 5.1 MPa for Brick (54.1x).

Which is lighter, Aluminum 6061-T6 or Brick?

Brick is lighter: 2,082 kg/m³ against 2,700 kg/m³ for Aluminum 6061-T6.

Which is lighter for the same job, Aluminum 6061-T6 or Brick?

For the same stiffness or strength: Aluminum 6061-T6 is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 6061-T6Brick
Strong rod or tielighter41.7x heavier
Strong beamlighter11x heavier
Strong panel or platelighter5.67x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Aluminum 6061-T6 or Brick?

Aluminum 6061-T6 conducts heat better: 167 W/m·K against 1.02 W/m·K for Brick.

Which expands less with temperature?

Brick expands less: 7.2 µm/m·K against 23.6 µm/m·K for Aluminum 6061-T6.

Related comparisons