Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: Kaiser Aluminum, BASF Forward AM, U.S. Department of Defense, INEOS Styrolution
Aluminum 6061-T6
6061-T6/T651, Kaiser Aluminum typical properties; Poisson from MIL-HDBK-5J
FDM HIPS
BASF Forward AM (BASF 3D Printing Solutions) Ultrafuse HiPS, TDS v2.2 (13.11.2019), printed specimens, XY 'Flat'. Specimen print settings are not stated; recommended processing on the sheet: nozzle 240-260 °C, bed 100-120 °C, 40-80 mm/s. Product is discontinued (Forward AM product page) but the TDS is still served by Forward AM.
1
Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 6061-T6 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 6061-T6 · Ultimate tensile strength: typicalAluminum 6061-T6 · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum 6061-T6 · Young's modulus (stiffness): typicalAluminum 6061-T6 · Density: nominalAluminum 6061-T6 · Thermal conductivity: typical, 20 °CAluminum 6061-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 6061-T6 · Specific heat: typical, at 100 °CAluminum 6061-T6 · Melting point: solidus-liquidus
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 6061-T6 · Poisson's ratio: typical (handbook physical constant)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM HIPS is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 6061-T6 stronger than FDM HIPS?
Aluminum 6061-T6 is stronger: its yield strength is 276 MPa against tensile strength 18.4 MPa for FDM HIPS (15x).
Which is lighter, Aluminum 6061-T6 or FDM HIPS?
FDM HIPS is lighter: 1,023 kg/m³ against 2,700 kg/m³ for Aluminum 6061-T6.
Which is stiffer, Aluminum 6061-T6 or FDM HIPS?
Aluminum 6061-T6 is stiffer: Young's modulus 68.3 GPa against 1.59 GPa for FDM HIPS, so the same part in Aluminum 6061-T6 deflects less under the same load.
Which is lighter for the same job, Aluminum 6061-T6 or FDM HIPS?
For the same stiffness or strength: Aluminum 6061-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 6061-T6
FDM HIPS
Stiff rod or tie (tension)
lighter
16.3x heavier
Stiff beam (bending)
lighter
2.48x heavier
Stiff panel or plate
lighter
33% heavier
Strong rod or tie
lighter
5.68x heavier
Strong beam
lighter
2.3x heavier
Strong panel or plate
lighter
47% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 6061-T6 or FDM HIPS?
Aluminum 6061-T6 stretches further before it breaks: 17% elongation at break against 1.4% for FDM HIPS.
Thermal
Which conducts heat better, Aluminum 6061-T6 or FDM HIPS?
Aluminum 6061-T6 conducts heat better: 167 W/m·K against 0.17 W/m·K for FDM HIPS.
Which expands less with temperature?
Aluminum 6061-T6 expands less: 23.6 µm/m·K against 80 µm/m·K for FDM HIPS.