Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: Kaiser Aluminum, Celanese, U.S. Department of Defense
Aluminum 6061-T6
6061-T6/T651, Kaiser Aluminum typical properties; Poisson from MIL-HDBK-5J
Plastic UHMWPE
Celanese GUR 4120 (avg. molecular weight 4.7x10^6 g/mol), typical values on compression-molded specimens; CTE and thermal conductivity from Celanese's generic UHMWPE guide (grade not named)
1
Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 6061-T6 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 6061-T6 · Ultimate tensile strength: typicalAluminum 6061-T6 · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum 6061-T6 · Young's modulus (stiffness): typicalAluminum 6061-T6 · Density: nominalAluminum 6061-T6 · Thermal conductivity: typical, 20 °CAluminum 6061-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 6061-T6 · Specific heat: typical, at 100 °CAluminum 6061-T6 · Melting point: solidus-liquidus
2
GUR UHMW-PE Overview (GUR-015)CelanesePlastic UHMWPE · Yield strength: typical, tensile stress at yield ISO 527, 50 mm/minPlastic UHMWPE · Ultimate tensile strength: typical, tensile stress at break ISO 527, 50 mm/minPlastic UHMWPE · Elongation at break: typical, nominal elongation at break ISO 527Plastic UHMWPE · Young's modulus (stiffness): typical, tensile modulus ISO 527, 1 mm/minPlastic UHMWPE · Density: typicalPlastic UHMWPE · Melting point: DSC 10 K/minPlastic UHMWPE · Max service temperature: recommended max constant operating temperature
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 6061-T6 · Poisson's ratio: typical (handbook physical constant)
4
GUR UHMW-PE Polymer Guide (GUR-003)Celanesearchived copyPlastic UHMWPE · Thermal conductivity: typical, unfilled (narrative value, generic Celanese UHMWPE)Plastic UHMWPE · Thermal expansion: typical, 20 to 100 °C (generic Celanese UHMWPE)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 6061-T6 stronger than Plastic UHMWPE?
Aluminum 6061-T6 is stronger: its yield strength is 276 MPa against 20 MPa for Plastic UHMWPE (13.8x).
Which is lighter, Aluminum 6061-T6 or Plastic UHMWPE?
Plastic UHMWPE is lighter: 930 kg/m³ against 2,700 kg/m³ for Aluminum 6061-T6.
Which is stiffer, Aluminum 6061-T6 or Plastic UHMWPE?
Aluminum 6061-T6 is stiffer: Young's modulus 68.3 GPa against 0.66 GPa for Plastic UHMWPE, so the same part in Aluminum 6061-T6 deflects less under the same load.
Which is lighter for the same job, Aluminum 6061-T6 or Plastic UHMWPE?
For the same stiffness or strength: Aluminum 6061-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 6061-T6
Plastic UHMWPE
Stiff rod or tie (tension)
lighter
35.6x heavier
Stiff beam (bending)
lighter
3.5x heavier
Stiff panel or plate
lighter
1.62x heavier
Strong rod or tie
lighter
4.75x heavier
Strong beam
lighter
1.98x heavier
Strong panel or plate
lighter
28% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 6061-T6 or Plastic UHMWPE?
Plastic UHMWPE stretches further before it breaks: 465% elongation at break against 17% for Aluminum 6061-T6.
Thermal
Which conducts heat better, Aluminum 6061-T6 or Plastic UHMWPE?
Aluminum 6061-T6 conducts heat better: 167 W/m·K against 0.4 W/m·K for Plastic UHMWPE.
Which expands less with temperature?
Aluminum 6061-T6 expands less: 23.6 µm/m·K against 200 µm/m·K for Plastic UHMWPE.