Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Kaiser Aluminum, Formlabs, U.S. Department of Defense
Aluminum 6061-T6
6061-T6/T651, Kaiser Aluminum typical properties; Poisson from MIL-HDBK-5J
SLA Resin Elastic 50A
Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.
1
Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 6061-T6 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 6061-T6 · Ultimate tensile strength: typicalAluminum 6061-T6 · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum 6061-T6 · Young's modulus (stiffness): typicalAluminum 6061-T6 · Density: nominalAluminum 6061-T6 · Thermal conductivity: typical, 20 °CAluminum 6061-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 6061-T6 · Specific heat: typical, at 100 °CAluminum 6061-T6 · Melting point: solidus-liquidus
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 6061-T6 · Poisson's ratio: typical (handbook physical constant)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 6061-T6 stronger than SLA Resin Elastic 50A?
Aluminum 6061-T6 is stronger: its yield strength is 276 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (81.2x).
Which is lighter, Aluminum 6061-T6 or SLA Resin Elastic 50A?
SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 2,700 kg/m³ for Aluminum 6061-T6.
Which is lighter for the same job, Aluminum 6061-T6 or SLA Resin Elastic 50A?
For the same stiffness or strength: Aluminum 6061-T6 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 6061-T6
SLA Resin Elastic 50A
Strong rod or tie
lighter
30.4x heavier
Strong beam
lighter
7.01x heavier
Strong panel or plate
lighter
3.37x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 6061-T6 or SLA Resin Elastic 50A?
SLA Resin Elastic 50A stretches further before it breaks: 160% elongation at break against 17% for Aluminum 6061-T6.