Mechanical
Yield strength276MPasourcetypical, 0.2% offset, .500 in dia specimen221MPasourcetypical
Ultimate tensile strength310MPasourcetypical283MPasourcetypical
Elongation at break17%sourcetypical, in 4D, 0.500 in dia specimen10%sourcetypical, in 2 in.
Young's modulus (stiffness)68.3GPasourcetypical85.5GPasourcetypical25% stiffer
Density2,700kg/m³sourcenominal6,600kg/m³sourcetypical
Strength to weight102kN·m/kg3.05x higher33.5kN·m/kg
Stiffness to weight25.3MN·m/kg1.95x higher13MN·m/kg
Poisson's ratio0.33sourcetypical (handbook physical constant)0.27sourcetypical, Zamak 3 hot-chamber die cast
Shear modulus25.7GPa33.7GPa31% stiffer in shear
Bulk modulus67GPa62GPa
Speed of sound5,030m/s3,599m/s
Thermal
Thermal conductivity167W/m·Ksourcetypical, 20 °C113W/m·Ksourcetypical
Thermal expansion23.6µm/m·Ksourcetypical, mean 20-100 °C27.4µm/m·Ksourcetypical
100 mm part over a 50 °C swing118µm growth16% less137µm growth
Specific heat896J/kg·Ksourcetypical, at 100 °C419J/kg·Ksourcetypical
Heats up and cools (diffusivity)69mm²/s1.69x faster40.9mm²/s
Thermal shock resistance19,159W/m2.46x more resistant7,782W/m
Melting point582–652°Csourcesolidus-liquidus381–387°Csourcemelting range
Values for6061-T6/T651, Kaiser Aluminum typical properties; Poisson from MIL-HDBK-5JZamak 3 (ASTM B86 die cast), Nathan Trotter (zinc alloy producer) technical data sheet, typical values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum 6061-T6 stronger than Zinc Zamak 3?

Aluminum 6061-T6 is stronger: its yield strength is 276 MPa against 221 MPa for Zinc Zamak 3 (25%).

Which is lighter, Aluminum 6061-T6 or Zinc Zamak 3?

Aluminum 6061-T6 is lighter: 2,700 kg/m³ against 6,600 kg/m³ for Zinc Zamak 3.

Which is stiffer, Aluminum 6061-T6 or Zinc Zamak 3?

Zinc Zamak 3 is stiffer: Young's modulus 85.5 GPa against 68.3 GPa for Aluminum 6061-T6, so the same part in Zinc Zamak 3 deflects less under the same load.

Which is lighter for the same job, Aluminum 6061-T6 or Zinc Zamak 3?

For the same stiffness or strength: Aluminum 6061-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 6061-T6Zinc Zamak 3
Stiff rod or tie (tension)lighter1.95x heavier
Stiff beam (bending)lighter2.18x heavier
Stiff panel or platelighter2.27x heavier
Strong rod or tielighter3.05x heavier
Strong beamlighter2.83x heavier
Strong panel or platelighter2.73x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Aluminum 6061-T6 or Zinc Zamak 3?

Aluminum 6061-T6 conducts heat better: 167 W/m·K against 113 W/m·K for Zinc Zamak 3.

Which expands less with temperature?

Aluminum 6061-T6 expands less: 23.6 µm/m·K against 27.4 µm/m·K for Zinc Zamak 3.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 6061-T6Zinc Zamak 3
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 6061-T6Zinc Zamak 3
Strength against density

Related comparisons