Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Kaiser Aluminum, Formlabs, Hydro
Aluminum 6063-T6
6063-T6 extruded tube, Kaiser Aluminum Tube & Pipe Alloy 6063 Technical Data (Rev. 05/06), typical properties; specific heat from Hydro EN AW-6063 extruded-products datasheet (Rev.4, 03/2023).
SLA Resin Standard
Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.
Clear Resin V5 Technical Data Sheet (2024)Formlabsarchived copySLA Resin Standard · Ultimate tensile strength: typicalSLA Resin Standard · Flexural strength: typicalSLA Resin Standard · Elongation at break: typicalSLA Resin Standard · Young's modulus (stiffness): typicalSLA Resin Standard · Max service temperature: HDT 1.8 MPa
3
Clear Resin V5 Technical Data Sheet (web edition)FormlabsSLA Resin Standard · Density: typical, post-cured (same for 5 min ambient and 15 min at 60 °C), ASTM D792
4
Thermal Properties of Selected Formlabs SLA ResinsFormlabsSLA Resin Standard · Thermal conductivity: typical, post-cured, ASTM E1530SLA Resin Standard · Thermal expansion: mean -30 to 140 °C, post-cured (5 min ambient cure), TMA ASTM E831SLA Resin Standard · Specific heat: typical, 25 °C, post-cured (5 min ambient cure), DSC ASTM E1269
5
Technical Datasheet, Extruded Products: Alloy EN AW-6063 (Rev. 4, 2023)Hydroarchived copyAluminum 6063-T6 · Specific heat: typical, 20 °C (Hydro EN AW-6063)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 6063-T6 stronger than SLA Resin Standard?
Aluminum 6063-T6 is stronger: its yield strength is 215 MPa against tensile strength 60 MPa for SLA Resin Standard (3.58x).
Which is lighter, Aluminum 6063-T6 or SLA Resin Standard?
SLA Resin Standard is lighter: 1,210 kg/m³ against 2,700 kg/m³ for Aluminum 6063-T6.
Which is stiffer, Aluminum 6063-T6 or SLA Resin Standard?
Aluminum 6063-T6 is stiffer: Young's modulus 69 GPa against 2.75 GPa for SLA Resin Standard, so the same part in Aluminum 6063-T6 deflects less under the same load.
Which is lighter for the same job, Aluminum 6063-T6 or SLA Resin Standard?
For the same stiffness or strength: Aluminum 6063-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam; SLA Resin Standard is lighter for a strong panel or plate.
Part that must be
Aluminum 6063-T6
SLA Resin Standard
Stiff rod or tie (tension)
lighter
11.2x heavier
Stiff beam (bending)
lighter
2.24x heavier
Stiff panel or plate
lighter
31% heavier
Strong rod or tie
lighter
1.61x heavier
Strong beam
lighter
5% heavier
Strong panel or plate
18% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 6063-T6 or SLA Resin Standard?
Aluminum 6063-T6 stretches further before it breaks: 12% elongation at break against 8% for SLA Resin Standard.
Thermal
Which conducts heat better, Aluminum 6063-T6 or SLA Resin Standard?
Aluminum 6063-T6 conducts heat better: 201 W/m·K against 0.54 W/m·K for SLA Resin Standard.
Which expands less with temperature?
Aluminum 6063-T6 expands less: 23.4 µm/m·K against 114 µm/m·K for SLA Resin Standard.