Materials / Compare
Aluminum 7050-T7451 vs. Ceramic Aluminum Nitride Compare Aluminum 7050-T7451 vs. Ceramic Aluminum Nitride strength, stiffness, weight and thermal properties.
Change either side
Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Aluminum 7050-T7451 Wrought Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Ceramic Aluminum Nitride Sintered ceramic (pressed and fired) Try it on a partA sample part to run stress or thermal on, free in your browser Open in LessCAD Open in LessCAD Mechanical Yield strength 469 MPa source typical, longitudinal, 0.2% offset not sourced Ultimate tensile strength 524 MPa source typical, longitudinal not sourced Flexural strength not sourced 310 MPa source 3-point bending strength (JIS R 1601) Elongation at break 11 % source typical, longitudinal not sourced Young's modulus (stiffness) 70.3 GPa source typical 320 GPa source typical (JIS R 1602) Density 2,830 kg/m³ source nominal 3,400 kg/m³ source typical (JIS R 1634) Strength to weight 166 kN·m/kg not sourced Stiffness to weight 24.8 MN·m/kg 94.1 MN·m/kg 3.79x higher Poisson's ratio 0.33 source typical (handbook physical constant) 0.24 source typical (JIS R 1602) Shear modulus 26.4 GPa 129 GPa 4.88x stiffer in shear Bulk modulus 68.9 GPa 205 GPa Speed of sound 4,984 m/s 9,701 m/s Thermal Thermal conductivity 157 W/m·K source typical, 20 °C 150 W/m·K source typical (JIS R 1611) Thermal expansion 23.5 µm/m·K source typical, mean 20-100 °C 4.6 µm/m·K source mean, 40-400 °C (JIS R 1618) 100 mm part over a 50 °C swing 118 µm growth 23 µm growth 5.11x less Specific heat 860 J/kg·K source typical, at 100 °C 710 J/kg·K source typical (JIS R 1611) Heats up and cools (diffusivity) 64.5 mm²/s 4% faster 62.1 mm²/s Thermal shock resistance 29,862 W/m not sourced Melting point 524–635 °C source melting range not sourced Values for 7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J KYOCERA AN216A dense sintered aluminium nitride, typical values; KYOCERA Fineceramics Europe data sheet 2023.04.03
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions Which is lighter, Aluminum 7050-T7451 or Ceramic Aluminum Nitride? Aluminum 7050-T7451 is lighter: 2,830 kg/m³ against 3,400 kg/m³ for Ceramic Aluminum Nitride.
Which is stiffer, Aluminum 7050-T7451 or Ceramic Aluminum Nitride? Ceramic Aluminum Nitride is stiffer: Young's modulus 320 GPa against 70.3 GPa for Aluminum 7050-T7451, so the same part in Ceramic Aluminum Nitride deflects less under the same load.
Which is lighter for the same job, Aluminum 7050-T7451 or Ceramic Aluminum Nitride? For the same stiffness or strength: Ceramic Aluminum Nitride is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.
Part that must be Aluminum 7050-T7451 Ceramic Aluminum Nitride Stiff rod or tie (tension) 3.79x heavier lighter Stiff beam (bending) 1.78x heavier lighter Stiff panel or plate 38% heavier lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which conducts heat better, Aluminum 7050-T7451 or Ceramic Aluminum Nitride? Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 150 W/m·K for Ceramic Aluminum Nitride.
Which expands less with temperature? Ceramic Aluminum Nitride expands less: 4.6 µm/m·K against 23.5 µm/m·K for Aluminum 7050-T7451.
Among 72 materials 1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel PCB Laminate FR-4 Silicon Ceramic Alumina 96% Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Aluminum 7050-T7451 Ceramic Aluminum Nitride Stiffness against density 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Rubber Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick PCB Laminate FR-4 Silicon Ceramic Alumina 96% Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Aluminum 7050-T7451 Strength against density