Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Technical Bulletin ATS-129: Properties of Soda-Lime Silica Float Glass (2025)Pilkington North Americaarchived copyGlass · Ultimate tensile strength: typical mean surface tensile stress at fracture (MOR), 60 s load, weathered, 50% breakage probabilityGlass · Flexural strength: mean MOR (same value as tensile)Glass · Young's modulus (stiffness): typicalGlass · Density: typicalGlass · Poisson's ratio: typicalGlass · Thermal conductivity: typical at 75 FGlass · Thermal expansion: typical, 75-575 FGlass · Specific heat: typical at 75 FGlass · Max service temperature: strain point (ASTM C336) - stress-relaxation onset, not a rated service limit
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 7050-T7451 stronger than Glass?
Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against tensile strength 41 MPa for Glass (11.4x).
Which is lighter, Aluminum 7050-T7451 or Glass?
Glass is lighter: 2,500 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.
Which is stiffer, Aluminum 7050-T7451 or Glass?
Glass is stiffer: Young's modulus 72 GPa against 70.3 GPa for Aluminum 7050-T7451, so the same part in Glass deflects less under the same load.
Which is lighter for the same job, Aluminum 7050-T7451 or Glass?
For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a strong rod or tie, strong beam, strong panel or plate; Glass is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.
Part that must be
Aluminum 7050-T7451
Glass
Stiff rod or tie (tension)
16% heavier
lighter
Stiff beam (bending)
15% heavier
lighter
Stiff panel or plate
14% heavier
lighter
Strong rod or tie
lighter
10.1x heavier
Strong beam
lighter
4.48x heavier
Strong panel or plate
lighter
2.99x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Aluminum 7050-T7451 or Glass?
Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 0.937 W/m·K for Glass.
Which expands less with temperature?
Glass expands less: 8.3 µm/m·K against 23.5 µm/m·K for Aluminum 7050-T7451.