Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 1018 · Young's modulus (stiffness): base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Density: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Aluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)Steel AISI 1018 · Poisson's ratio: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Thermal conductivity: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Specific heat: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
4
S275JR Steel GradeOvakoSteel AISI 1018 · Thermal expansion: base material: unalloyed carbon steel, Ovako family table (S275JR, 'none alloyed structural steels', C <= 0.21%); mean 20-300 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 7050-T7451 stronger than Steel AISI 1018?
Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against 372 MPa for Steel AISI 1018 (26%).
Which is lighter, Aluminum 7050-T7451 or Steel AISI 1018?
Aluminum 7050-T7451 is lighter: 2,830 kg/m³ against 7,861 kg/m³ for Steel AISI 1018.
Which is stiffer, Aluminum 7050-T7451 or Steel AISI 1018?
Steel AISI 1018 is stiffer: Young's modulus 200 GPa against 70.3 GPa for Aluminum 7050-T7451, so the same part in Steel AISI 1018 deflects less under the same load.
Which is lighter for the same job, Aluminum 7050-T7451 or Steel AISI 1018?
For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Steel AISI 1018 is lighter for a stiff rod or tie (tension).
Part that must be
Aluminum 7050-T7451
Steel AISI 1018
Stiff rod or tie (tension)
2% heavier
lighter
Stiff beam (bending)
lighter
1.65x heavier
Stiff panel or plate
lighter
1.96x heavier
Strong rod or tie
lighter
3.5x heavier
Strong beam
lighter
3.24x heavier
Strong panel or plate
lighter
3.12x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 7050-T7451 or Steel AISI 1018?
Steel AISI 1018 stretches further before it breaks: 15% elongation at break against 11% for Aluminum 7050-T7451.
Thermal
Which conducts heat better, Aluminum 7050-T7451 or Steel AISI 1018?
Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 51.9 W/m·K for Steel AISI 1018.
Which expands less with temperature?
Steel AISI 1018 expands less: 12 µm/m·K against 23.5 µm/m·K for Aluminum 7050-T7451.