Materials / Compare

Aluminum 7050-T7451 vs. Steel AISI 4340

Compare Aluminum 7050-T7451 vs. Steel AISI 4340 strength, stiffness, weight and thermal properties.

Aluminum 7050-T7451Wrought
Steel AISI 4340Wrought
MechanicalAluminum 7050-T7451Steel AISI 4340
Yield strength469MPa11,035MPa22.21x stronger
Ultimate tensile strength524MPa11,140MPa22.18x stronger
Elongation at break11%118%21.64x more ductile
Young's modulus (stiffness)70.3GPa1200GPa3
Density2,830kg/m³12.77x lighter7,840kg/m³2
Strength to weight166kN·m/kg26% higher132kN·m/kg
Stiffness to weight24.8MN·m/kg25.5MN·m/kg3% higher
Poisson's ratio0.3330.323
Shear modulus26.4GPa75.7GPa2.87x stiffer in shear
Bulk modulus68.9GPa185GPa2.69x higher
Speed of sound4,984m/s5,049m/s1% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Steel AISI 4340
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Steel AISI 4340
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 7050-T7451Steel AISI 4340
Thermal conductivity157W/m·K14.19x more heat through a fin37.5W/m·K2
Thermal expansion23.5µm/m·K1mean11.3µm/m·K22.08x less
100 mm part over a 50 °C swing118µm growth56.5µm growth2.08x less
Specific heat860J/kg·K11.92x higher448J/kg·K2
Heats up and cools (diffusivity)64.5mm²/s6.05x faster10.7mm²/s
Thermal shock resistance29,862W/m2.56x more resistant11,678W/m
Melting pointmelting range524–635°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Steel AISI 4340
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Steel AISI 4340
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Kaiser Aluminum, Carpenter Technology, U.S. Department of Defense
Aluminum 7050-T7451
7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J
Steel AISI 4340
Carpenter (Latrobe) Lescalloy 4340 VAC-ARC datasheet; mechanical row for 1100 °F temper; physical properties grade-level
  1. 1
    Alloy 7050 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 7050-T7451 · Yield strength: typical, longitudinal, 0.2% offsetAluminum 7050-T7451 · Ultimate tensile strength: typical, longitudinalAluminum 7050-T7451 · Elongation at break: typical, longitudinalAluminum 7050-T7451 · Young's modulus (stiffness): typicalAluminum 7050-T7451 · Density: nominalAluminum 7050-T7451 · Thermal conductivity: typical, 20 °CAluminum 7050-T7451 · Thermal expansion: typical, mean 20-100 °CAluminum 7050-T7451 · Specific heat: typical, at 100 °CAluminum 7050-T7451 · Melting point: melting range
  2. 2
    Lescalloy 4340 VAC-ARC Data SheetCarpenter Technologyarchived copySteel AISI 4340 · Yield strength: typical, transverseSteel AISI 4340 · Ultimate tensile strength: typical, transverseSteel AISI 4340 · Elongation at break: typical, transverseSteel AISI 4340 · Density: typicalSteel AISI 4340 · Thermal conductivity: typicalSteel AISI 4340 · Thermal expansion: mean, -18 to 93 °CSteel AISI 4340 · Specific heat: typical
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 4340 · Young's modulus (stiffness): MIL-HDBK-5J design value (AISI 4340, quenched and tempered)Aluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)Steel AISI 4340 · Poisson's ratio: MIL-HDBK-5J design value (AISI 4340, quenched and tempered)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 7050-T7451 stronger than Steel AISI 4340?

Steel AISI 4340 is stronger: its yield strength is 1,035 MPa against 469 MPa for Aluminum 7050-T7451 (2.21x).

Which is lighter, Aluminum 7050-T7451 or Steel AISI 4340?

Aluminum 7050-T7451 is lighter: 2,830 kg/m³ against 7,840 kg/m³ for Steel AISI 4340.

Which is stiffer, Aluminum 7050-T7451 or Steel AISI 4340?

Steel AISI 4340 is stiffer: Young's modulus 200 GPa against 70.3 GPa for Aluminum 7050-T7451, so the same part in Steel AISI 4340 deflects less under the same load.

Which is lighter for the same job, Aluminum 7050-T7451 or Steel AISI 4340?

For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Steel AISI 4340 is lighter for a stiff rod or tie (tension).

Part that must beAluminum 7050-T7451Steel AISI 4340
Stiff rod or tie (tension)3% heavierlighter
Stiff beam (bending)lighter1.64x heavier
Stiff panel or platelighter1.96x heavier
Strong rod or tielighter26% heavier
Strong beamlighter1.63x heavier
Strong panel or platelighter1.86x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 7050-T7451 or Steel AISI 4340?

Steel AISI 4340 stretches further before it breaks: 18% elongation at break against 11% for Aluminum 7050-T7451.

Thermal

Which conducts heat better, Aluminum 7050-T7451 or Steel AISI 4340?

Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 37.5 W/m·K for Steel AISI 4340.

Which expands less with temperature?

Steel AISI 4340 expands less: 11.3 µm/m·K against 23.5 µm/m·K for Aluminum 7050-T7451.