Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Kaiser Aluminum, UltiMaker, U.S. Department of Defense, Covestro
Aluminum
6061-T6/T651, Kaiser Aluminum typical properties (sheet, coil & plate datasheet); Poisson from MIL-HDBK-5J
FDM Polycarbonate
Ultimaker PC, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 20, 2022.
1
Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum · Ultimate tensile strength: typicalAluminum · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum · Young's modulus (stiffness): typicalAluminum · Density: nominalAluminum · Thermal conductivity: typical, 20 °CAluminum · Thermal expansion: typical, mean 20-100 °CAluminum · Specific heat: typical, at 100 °CAluminum · Melting point: solidus-liquidus
2
Ultimaker PC Technical Data Sheet, v5.00UltiMakerarchived copyFDM Polycarbonate · Yield strength: typicalFDM Polycarbonate · Ultimate tensile strength: typical, peak stress (= stress at yield)FDM Polycarbonate · Flexural strength: typicalFDM Polycarbonate · Elongation at break: typicalFDM Polycarbonate · Young's modulus (stiffness): typicalFDM Polycarbonate · Density: rangeFDM Polycarbonate · Glass transition: typicalFDM Polycarbonate · Max service temperature: HDT 0.455 MPa (printed specimens)
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum · Poisson's ratio: typical (handbook physical constant)
4
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyFDM Polycarbonate · Poisson's ratio: base material: polycarbonate family typical (Covestro Part and Mold Design guide, Table 3-1)
5
Makrolon 2405 Technical Data SheetCovestroFDM Polycarbonate · Thermal conductivity: base material: Covestro Makrolon 2405 injection-molding PC, typical, through-plane, 23 °CFDM Polycarbonate · Thermal expansion: base material: Covestro Makrolon 2405 injection-molding PC, typical, 23-55 °C, parallel
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM Polycarbonate is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum stronger than FDM Polycarbonate?
Aluminum is stronger: its yield strength is 276 MPa against 53.3 MPa for FDM Polycarbonate (5.18x).
Which is lighter, Aluminum or FDM Polycarbonate?
FDM Polycarbonate is lighter: 1,190 kg/m³ against 2,700 kg/m³ for Aluminum.
Which is stiffer, Aluminum or FDM Polycarbonate?
Aluminum is stiffer: Young's modulus 68.3 GPa against 2.39 GPa for FDM Polycarbonate, so the same part in Aluminum deflects less under the same load.
Which is lighter for the same job, Aluminum or FDM Polycarbonate?
For the same stiffness or strength: Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam.
Part that must be
Aluminum
FDM Polycarbonate
Stiff rod or tie (tension)
lighter
12.6x heavier
Stiff beam (bending)
lighter
2.35x heavier
Stiff panel or plate
lighter
35% heavier
Strong rod or tie
lighter
2.28x heavier
Strong beam
lighter
32% heavier
Strong panel or plate
about equal
about equal
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum or FDM Polycarbonate?
Aluminum stretches further before it breaks: 17% elongation at break against 9.2% for FDM Polycarbonate.
Thermal
Which conducts heat better, Aluminum or FDM Polycarbonate?
Aluminum conducts heat better: 167 W/m·K against 0.2 W/m·K for FDM Polycarbonate.
Which expands less with temperature?
Aluminum expands less: 23.6 µm/m·K against 65 µm/m·K for FDM Polycarbonate.