Materials / Compare

Brass C360 vs. Plastic PMMA

Compare Brass C360 vs. Plastic PMMA strength, stiffness, weight and thermal properties.

Brass C360Wrought
Plastic PMMABulk polymer (molded or machined)
MechanicalBrass C360Plastic PMMA
Yield strength310MPa1not given (tensile used)
Ultimate tensile strength400MPa15x stronger80MPa2
Compressive strengthnot sourced110MPa2
Flexural strengthnot sourced115MPa2
Elongation at break25%14.55x more ductile5.5%2
Young's modulus (stiffness)96.5GPa129.2x stiffer3.3GPa2
Density8,498kg/m³11,190kg/m³27.14x lighter
Strength to weight36.5kN·m/kg67.2kN·m/kg1.84x higher
Stiffness to weight11.4MN·m/kg4.09x higher2.77MN·m/kg
Poisson's ratiobase material0.3430.372
Shear modulus36GPa29.9x stiffer in shear1.2GPa
Bulk modulus101GPa23.8x higher4.23GPa
Speed of sound3,370m/s2.02x faster1,665m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360Plastic PMMA
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360Plastic PMMA
Strength against densityHigher and further left: stronger for its weight
ThermalBrass C360Plastic PMMA
Thermal conductivity116W/m·K1611x more heat through a fin0.19W/m·K2
Thermal expansion20.5µm/m·K13.41x less0-50 °C70µm/m·K2
100 mm part over a 50 °C swing103µm growth3.41x less350µm growth
Specific heat377J/kg·K11,470J/kg·K23.9x higher
Heats up and cools (diffusivity)36.2mm²/s334x faster0.109mm²/s
Thermal shock resistance11,997W/m289x more resistant41.5W/m
Melting pointsolidus-liquidus888–899°C1not sourced
Max service temperaturenot sourced80°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360Plastic PMMA
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C360Plastic PMMA
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Copper Development Association, Röhm, Wieland
Brass C360
C36000 free-cutting brass, H02 half-hard rod 1 in. section (20% cold work), copper.org typical values
Plastic PMMA
Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)
  1. 1
    C36000 Alloy (copper.org)Copper Development Associationarchived copyBrass C360 · Yield strength: typical, 0.5% extension under loadBrass C360 · Ultimate tensile strength: typicalBrass C360 · Elongation at break: typical, 1 in. rodBrass C360 · Young's modulus (stiffness): typical, temper-independentBrass C360 · Density: nominalBrass C360 · Thermal conductivity: typical, 20 °CBrass C360 · Thermal expansion: typical, mean 20-300 °CBrass C360 · Specific heat: typical, 20 °CBrass C360 · Melting point: solidus-liquidus
  2. 2
    PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
  3. 3
    Wieland-Z30 (CuZn39Pb2, C37700) Data SheetWielandarchived copyBrass C360 · Poisson's ratio: base material: leaded free-machining brass CuZn39Pb2 (C37700), Wieland-Z30 rolled products, reference value at room temperature

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Brass C360 stronger than Plastic PMMA?

Brass C360 is stronger: its yield strength is 310 MPa against tensile strength 80 MPa for Plastic PMMA (3.88x).

Which is lighter, Brass C360 or Plastic PMMA?

Plastic PMMA is lighter: 1,190 kg/m³ against 8,498 kg/m³ for Brass C360.

Which is stiffer, Brass C360 or Plastic PMMA?

Brass C360 is stiffer: Young's modulus 96.5 GPa against 3.3 GPa for Plastic PMMA, so the same part in Brass C360 deflects less under the same load.

Which is lighter for the same job, Brass C360 or Plastic PMMA?

For the same stiffness or strength: Brass C360 is lighter for a stiff rod or tie (tension); Plastic PMMA is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beBrass C360Plastic PMMA
Stiff rod or tie (tension)lighter4.09x heavier
Stiff beam (bending)32% heavierlighter
Stiff panel or plate2.32x heavierlighter
Strong rod or tie1.84x heavierlighter
Strong beam2.89x heavierlighter
Strong panel or plate3.63x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Brass C360 or Plastic PMMA?

Brass C360 stretches further before it breaks: 25% elongation at break against 5.5% for Plastic PMMA.

Thermal

Which conducts heat better, Brass C360 or Plastic PMMA?

Brass C360 conducts heat better: 116 W/m·K against 0.19 W/m·K for Plastic PMMA.

Which expands less with temperature?

Brass C360 expands less: 20.5 µm/m·K against 70 µm/m·K for Plastic PMMA.