Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
C10100 Alloy (copper.org)Copper Development Associationarchived copyCopper C10100 · Yield strength: typical, 0.5% extension under load, 0.04 in. flatCopper C10100 · Ultimate tensile strength: typical, 0.04 in. flatCopper C10100 · Elongation at break: typical, 0.04 in. flatCopper C10100 · Young's modulus (stiffness): typicalCopper C10100 · Density: nominalCopper C10100 · Thermal conductivity: typical, 20 °CCopper C10100 · Thermal expansion: typical, mean 20-100 °CCopper C10100 · Specific heat: typical, 20 °CCopper C10100 · Melting point: melting point (liquidus = solidus, pure copper)
2
Elektron AZ31B Sheet, Plate & Coil (Datasheet 482)Magnesium Elektronarchived copyMagnesium AZ31B-H24 · Yield strength: typical, H24, 0.5-6 mm, 0.2 % proof stressMagnesium AZ31B-H24 · Ultimate tensile strength: typical, H24, 0.5-6 mmMagnesium AZ31B-H24 · Elongation at break: typical, H24, 0.5-6 mm, gauge 5.65√AMagnesium AZ31B-H24 · Thermal conductivity: typical (temper/temperature not stated)Magnesium AZ31B-H24 · Thermal expansion: typical (temperature range not stated)Magnesium AZ31B-H24 · Specific heat: typical
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ31B-H24 · Young's modulus (stiffness): typical (handbook physical constant)Magnesium AZ31B-H24 · Density: nominalMagnesium AZ31B-H24 · Poisson's ratio: typical (handbook physical constant)Magnesium AZ31B-H24 · Max service temperature: stated application limit
4
Wieland-K09 (Cu-OFE, C10100) Data SheetWielandCopper C10100 · Poisson's ratio: reference value at room temperature (Wieland-K09 = Cu-OFE = C10100, rolled products)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Copper C10100 stronger than Magnesium AZ31B-H24?
Magnesium AZ31B-H24 is stronger: its yield strength is 220 MPa against 69 MPa for Copper C10100 (3.19x).
Which is lighter, Copper C10100 or Magnesium AZ31B-H24?
Magnesium AZ31B-H24 is lighter: 1,769 kg/m³ against 8,941 kg/m³ for Copper C10100.
Which is stiffer, Copper C10100 or Magnesium AZ31B-H24?
Copper C10100 is stiffer: Young's modulus 117 GPa against 44.8 GPa for Magnesium AZ31B-H24, so the same part in Copper C10100 deflects less under the same load.
Which is lighter for the same job, Copper C10100 or Magnesium AZ31B-H24?
For the same stiffness or strength: Magnesium AZ31B-H24 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Copper C10100
Magnesium AZ31B-H24
Stiff rod or tie (tension)
1.93x heavier
lighter
Stiff beam (bending)
3.12x heavier
lighter
Stiff panel or plate
3.67x heavier
lighter
Strong rod or tie
16.1x heavier
lighter
Strong beam
10.9x heavier
lighter
Strong panel or plate
9.02x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Copper C10100 or Magnesium AZ31B-H24?
Copper C10100 stretches further before it breaks: 45% elongation at break against 13% for Magnesium AZ31B-H24.
Thermal
Which conducts heat better, Copper C10100 or Magnesium AZ31B-H24?
Copper C10100 conducts heat better: 391 W/m·K against 76.9 W/m·K for Magnesium AZ31B-H24.
Which expands less with temperature?
Copper C10100 expands less: 16.9 µm/m·K against 26.8 µm/m·K for Magnesium AZ31B-H24.