Materials / Compare

Copper C10100 vs. Plastic ABS

Compare Copper C10100 vs. Plastic ABS strength, stiffness, weight and thermal properties.

Copper C10100Wrought
Plastic ABS3D printed (FDM)
MechanicalCopper C10100Plastic ABS
Yield strength69MPa11.81x stronger38.1MPa2
Ultimate tensile strength221MPa15.8x stronger38.1MPa2
Flexural strengthnot sourced61.1MPa2
Elongation at break45%19.78x more ductile4.6%2
Young's modulus (stiffness)117GPa159.7x stiffer1.96GPa2
Density8,941kg/m³11,100kg/m³28.13x lighter
Strength to weight7.72kN·m/kg34.6kN·m/kg4.49x higher
Stiffness to weight13.1MN·m/kg7.35x higher1.78MN·m/kg
Poisson's ratio0.343base material0.394
Shear modulus43.7GPa62x stiffer in shear0.706GPa
Bulk modulus122GPa41.1x higher2.97GPa
Speed of sound3,621m/s2.71x faster1,336m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C10100Plastic ABS
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C10100Plastic ABS
Strength against densityHigher and further left: stronger for its weight
ThermalCopper C10100Plastic ABS
Thermal conductivity391W/m·K12,301x more heat through a finbase material0.17W/m·K5
Thermal expansion16.9µm/m·K1base material80–110µm/m·K5
100 mm part over a 50 °C swing84.5µm growth5.62x less475µm growth
Specific heat385J/kg·K1not sourced
Heats up and cools (diffusivity)114mm²/snot sourced
Thermal shock resistance8,992W/m424x more resistant21.2W/m
Melting pointmelting point1,083°C1not sourced
Glass transitionnot sourced101°C2
Max service temperaturenot sourcedHDT 0.455 MPa86.6°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C10100Plastic ABS
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C10100Plastic ABS
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Copper Development Association, UltiMaker, Wieland, Covestro, INEOS Styrolution
Copper C10100
C10100 oxygen-free electronic (OFE) copper, annealed to 0.050 mm grain size (OS050), 0.04 in. flat products, copper.org typical values
Plastic ABS
Ultimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.
  1. 1
    C10100 Alloy (copper.org)Copper Development Associationarchived copyCopper C10100 · Yield strength: typical, 0.5% extension under load, 0.04 in. flatCopper C10100 · Ultimate tensile strength: typical, 0.04 in. flatCopper C10100 · Elongation at break: typical, 0.04 in. flatCopper C10100 · Young's modulus (stiffness): typicalCopper C10100 · Density: nominalCopper C10100 · Thermal conductivity: typical, 20 °CCopper C10100 · Thermal expansion: typical, mean 20-100 °CCopper C10100 · Specific heat: typical, 20 °CCopper C10100 · Melting point: melting point (liquidus = solidus, pure copper)
  2. 2
    Ultimaker ABS Technical Data Sheet, v5.00UltiMakerarchived copyPlastic ABS · Yield strength: typicalPlastic ABS · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic ABS · Flexural strength: typicalPlastic ABS · Elongation at break: typicalPlastic ABS · Young's modulus (stiffness): typicalPlastic ABS · Density: typicalPlastic ABS · Glass transition: typicalPlastic ABS · Max service temperature: HDT 0.455 MPa (printed specimens)
  3. 3
    Wieland-K09 (Cu-OFE, C10100) Data SheetWielandCopper C10100 · Poisson's ratio: reference value at room temperature (Wieland-K09 = Cu-OFE = C10100, rolled products)
  4. 4
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic ABS · Poisson's ratio: base material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)
  5. 5
    Terluran GP-22 (ABS) Product Data SheetINEOS StyrolutionPlastic ABS · Thermal conductivity: base material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typicalPlastic ABS · Thermal expansion: base material: INEOS Styrolution Terluran GP-22 injection-molding ABS, range

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic ABS is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Copper C10100 stronger than Plastic ABS?

Copper C10100 is stronger: its yield strength is 69 MPa against 38.1 MPa for Plastic ABS (1.81x).

Which is lighter, Copper C10100 or Plastic ABS?

Plastic ABS is lighter: 1,100 kg/m³ against 8,941 kg/m³ for Copper C10100.

Which is stiffer, Copper C10100 or Plastic ABS?

Copper C10100 is stiffer: Young's modulus 117 GPa against 1.96 GPa for Plastic ABS, so the same part in Copper C10100 deflects less under the same load.

Which is lighter for the same job, Copper C10100 or Plastic ABS?

For the same stiffness or strength: Copper C10100 is lighter for a stiff rod or tie (tension); Plastic ABS is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beCopper C10100Plastic ABS
Stiff rod or tie (tension)lighter7.35x heavier
Stiff beam (bending)5% heavierlighter
Stiff panel or plate2.08x heavierlighter
Strong rod or tie4.49x heavierlighter
Strong beam5.47x heavierlighter
Strong panel or plate6.04x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Copper C10100 or Plastic ABS?

Copper C10100 stretches further before it breaks: 45% elongation at break against 4.6% for Plastic ABS.

Thermal

Which conducts heat better, Copper C10100 or Plastic ABS?

Copper C10100 conducts heat better: 391 W/m·K against 0.17 W/m·K for Plastic ABS.

Which expands less with temperature?

Copper C10100 expands less: 16.9 µm/m·K against 95 µm/m·K for Plastic ABS.