Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Copper Development Association, UltiMaker, Wieland, Covestro
Copper C12200
C12200 phosphorus-deoxidized copper (DHP, the air-conditioning and refrigeration tube copper), tube annealed to 0.050 mm grain size (OS050), 0.065 in. wall, copper.org typical values
FDM Polycarbonate
Ultimaker PC, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 20, 2022.
1
C12200 Alloy (copper.org)Copper Development Associationarchived copyCopper C12200 · Yield strength: typical, 0.5% extension under load, 0.065 in. tubeCopper C12200 · Ultimate tensile strength: typical, 0.065 in. tubeCopper C12200 · Elongation at break: typical, 0.065 in. tubeCopper C12200 · Young's modulus (stiffness): typicalCopper C12200 · Density: nominalCopper C12200 · Thermal conductivity: typical, 20 °CCopper C12200 · Thermal expansion: typical, mean 20-100 °CCopper C12200 · Specific heat: typical, 20 °CCopper C12200 · Melting point: liquidus
2
Ultimaker PC Technical Data Sheet, v5.00UltiMakerarchived copyFDM Polycarbonate · Yield strength: typicalFDM Polycarbonate · Ultimate tensile strength: typical, peak stress (= stress at yield)FDM Polycarbonate · Flexural strength: typicalFDM Polycarbonate · Elongation at break: typicalFDM Polycarbonate · Young's modulus (stiffness): typicalFDM Polycarbonate · Density: rangeFDM Polycarbonate · Glass transition: typicalFDM Polycarbonate · Max service temperature: HDT 0.455 MPa (printed specimens)
3
Wieland-K19 (Cu-DHP, C12200) Data SheetWielandarchived copyCopper C12200 · Poisson's ratio: reference value at room temperature (Wieland-K19 = Cu-DHP = C12200, rolled products)
4
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyFDM Polycarbonate · Poisson's ratio: base material: polycarbonate family typical (Covestro Part and Mold Design guide, Table 3-1)
5
Makrolon 2405 Technical Data SheetCovestroFDM Polycarbonate · Thermal conductivity: base material: Covestro Makrolon 2405 injection-molding PC, typical, through-plane, 23 °CFDM Polycarbonate · Thermal expansion: base material: Covestro Makrolon 2405 injection-molding PC, typical, 23-55 °C, parallel
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM Polycarbonate is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Copper C12200 stronger than FDM Polycarbonate?
Copper C12200 is stronger: its yield strength is 69 MPa against 53.3 MPa for FDM Polycarbonate (29%).
Which is lighter, Copper C12200 or FDM Polycarbonate?
FDM Polycarbonate is lighter: 1,190 kg/m³ against 8,941 kg/m³ for Copper C12200.
Which is stiffer, Copper C12200 or FDM Polycarbonate?
Copper C12200 is stiffer: Young's modulus 117 GPa against 2.39 GPa for FDM Polycarbonate, so the same part in Copper C12200 deflects less under the same load.
Which is lighter for the same job, Copper C12200 or FDM Polycarbonate?
For the same stiffness or strength: Copper C12200 is lighter for a stiff rod or tie (tension); FDM Polycarbonate is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Copper C12200
FDM Polycarbonate
Stiff rod or tie (tension)
lighter
6.52x heavier
Stiff beam (bending)
7% heavier
lighter
Stiff panel or plate
2.05x heavier
lighter
Strong rod or tie
5.8x heavier
lighter
Strong beam
6.33x heavier
lighter
Strong panel or plate
6.6x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Copper C12200 or FDM Polycarbonate?
Copper C12200 stretches further before it breaks: 45% elongation at break against 9.2% for FDM Polycarbonate.
Thermal
Which conducts heat better, Copper C12200 or FDM Polycarbonate?
Copper C12200 conducts heat better: 339 W/m·K against 0.2 W/m·K for FDM Polycarbonate.
Which expands less with temperature?
Copper C12200 expands less: 16.9 µm/m·K against 65 µm/m·K for FDM Polycarbonate.