Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources7 documents: EOS GmbH, Celanese, Steel Construction Institute, Cleveland-Cliffs
DMLS 316L Stainless Steel
EOS StainlessSteel 316L (powder 9011-0032), EOS M 290, ParameterSet 316L 20µm Surface M290/400W, as manufactured, horizontal; ISO 6892-1
Plastic UHMWPE
Celanese GUR 4120 (avg. molecular weight 4.7x10^6 g/mol), typical values on compression-molded specimens; CTE and thermal conductivity from Celanese's generic UHMWPE guide (grade not named)
1
EOS StainlessSteel 316L Material Data SheetEOS GmbHarchived copyDMLS 316L Stainless Steel · Yield strength: typical, as manufactured, horizontalDMLS 316L Stainless Steel · Ultimate tensile strength: typical, as manufactured, horizontalDMLS 316L Stainless Steel · Elongation at break: typical at break, as manufactured, horizontalDMLS 316L Stainless Steel · Thermal expansion: mean 25-100 °C, ASTM E228
2
GUR UHMW-PE Overview (GUR-015)CelanesePlastic UHMWPE · Yield strength: typical, tensile stress at yield ISO 527, 50 mm/minPlastic UHMWPE · Ultimate tensile strength: typical, tensile stress at break ISO 527, 50 mm/minPlastic UHMWPE · Elongation at break: typical, nominal elongation at break ISO 527Plastic UHMWPE · Young's modulus (stiffness): typical, tensile modulus ISO 527, 1 mm/minPlastic UHMWPE · Density: typicalPlastic UHMWPE · Melting point: DSC 10 K/minPlastic UHMWPE · Max service temperature: recommended max constant operating temperature
3
EOS StainlessSteel 316L Material Data Sheet, M 280 and M 290 (2014)EOS GmbHarchived copyDMLS 316L Stainless Steel · Young's modulus (stiffness): typical, as built, horizontal (XY); EOSINT M280-400W / M290-400W, 316L_Surface 1.0, 20 µm (2014 sheet)
4
EOS StainlessSteel 316L Material Data Sheet, FlexLine, M 290 (2016)EOS GmbHarchived copyDMLS 316L Stainless Steel · Density: part density (ISO 3369, not labelled min or typical), EOS M 290, 40 µm FlexLine
5
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyDMLS 316L Stainless Steel · Poisson's ratio: base material: austenitic stainless steels incl. 1.4404 (316L), design value
6
316/316L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsDMLS 316L Stainless Steel · Thermal conductivity: base material: wrought 316/316L (Cleveland-Cliffs), at 100 °CDMLS 316L Stainless Steel · Specific heat: base material: wrought 316/316L (Cleveland-Cliffs), 0-100 °C
7
GUR UHMW-PE Polymer Guide (GUR-003)Celanesearchived copyPlastic UHMWPE · Thermal conductivity: typical, unfilled (narrative value, generic Celanese UHMWPE)Plastic UHMWPE · Thermal expansion: typical, 20 to 100 °C (generic Celanese UHMWPE)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS 316L Stainless Steel is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS 316L Stainless Steel stronger than Plastic UHMWPE?
DMLS 316L Stainless Steel is stronger: its yield strength is 530 MPa against 20 MPa for Plastic UHMWPE (26.5x).
Which is lighter, DMLS 316L Stainless Steel or Plastic UHMWPE?
Plastic UHMWPE is lighter: 930 kg/m³ against 7,900 kg/m³ for DMLS 316L Stainless Steel.
Which is stiffer, DMLS 316L Stainless Steel or Plastic UHMWPE?
DMLS 316L Stainless Steel is stiffer: Young's modulus 185 GPa against 0.66 GPa for Plastic UHMWPE, so the same part in DMLS 316L Stainless Steel deflects less under the same load.
Which is lighter for the same job, DMLS 316L Stainless Steel or Plastic UHMWPE?
For the same stiffness or strength: DMLS 316L Stainless Steel is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam; Plastic UHMWPE is lighter for a stiff panel or plate, strong panel or plate.
Part that must be
DMLS 316L Stainless Steel
Plastic UHMWPE
Stiff rod or tie (tension)
lighter
33x heavier
Stiff beam (bending)
lighter
1.97x heavier
Stiff panel or plate
30% heavier
lighter
Strong rod or tie
lighter
3.12x heavier
Strong beam
lighter
5% heavier
Strong panel or plate
1.65x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, DMLS 316L Stainless Steel or Plastic UHMWPE?
Plastic UHMWPE stretches further before it breaks: 465% elongation at break against 40% for DMLS 316L Stainless Steel.
Thermal
Which conducts heat better, DMLS 316L Stainless Steel or Plastic UHMWPE?
DMLS 316L Stainless Steel conducts heat better: 16.2 W/m·K against 0.4 W/m·K for Plastic UHMWPE.
Which expands less with temperature?
DMLS 316L Stainless Steel expands less: 15.7 µm/m·K against 200 µm/m·K for Plastic UHMWPE.