Compare DMLS AlSi10Mg Aluminum vs. Plastic Nylon PA66 strength, stiffness, weight and thermal properties.
| Mechanical | DMLS AlSi10Mg Aluminum | Plastic Nylon PA66 |
|---|---|---|
| Yield strength | 270MPa13.18x stronger | 85MPa2 |
| Ultimate tensile strength | 450MPa1 | not stated (yield given) |
| Elongation at break | 10.2%1 | 30%22.94x more ductile |
| Young's modulus (stiffness) | 72GPa324x stiffer | 3GPa2 |
| Density | 2,670kg/m³4 | 1,130kg/m³22.36x lighter |
| Strength to weight | 101kN·m/kg34% higher | 75.2kN·m/kg |
| Stiffness to weight | 27MN·m/kg10.2x higher | 2.65MN·m/kg |
| Poisson's ratio | base material0.335 | base material0.46 |
| Shear modulus | 27.1GPa25.3x stiffer in shear | 1.07GPa |
| Bulk modulus | 70.6GPa14.1x higher | 5GPa |
| Speed of sound | 5,193m/s3.19x faster | 1,629m/s |
| Thermal | DMLS AlSi10Mg Aluminum | Plastic Nylon PA66 |
|---|---|---|
| Thermal conductivity | 110W/m·K1333x more heat through a fin | 0.33W/m·K2 |
| Thermal expansion | mean 25-100 °C20µm/m·K14.9x less | longitudinal98µm/m·K2 |
| 100 mm part over a 50 °C swing | 100µm growth4.9x less | 490µm growth |
| Specific heat | base material963J/kg·K5 | 1,700J/kg·K2 |
| Heats up and cools (diffusivity) | 42.8mm²/s249x faster | 0.172mm²/s |
| Thermal shock resistance | 13,819W/m241x more resistant | 57.2W/m |
| Melting point | not sourced | DSC260°C2 |
| Max service temperature | not sourced | 101°C2 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources6 documents: EOS GmbH, BASF, Renishaw, U.S. Department of Defense, Covestro
- DMLS AlSi10Mg Aluminum
- EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10
- Plastic Nylon PA66
- BASF Ultramid A3K (PA66, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)
- 1EOS Aluminium AlSi10Mg Material Data SheetEOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Yield strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Ultimate tensile strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Elongation at break: typical at break, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Thermal conductivity: typical, as manufactured, horizontal (ISO 22007-2)DMLS AlSi10Mg Aluminum · Thermal expansion: mean 25-100 °C, ASTM E228
- 2Ultramid A3K Product InformationBASFPlastic Nylon PA66 · Yield strength: typical, dryPlastic Nylon PA66 · Elongation at break: nominal strain at break, dryPlastic Nylon PA66 · Young's modulus (stiffness): typical, dryPlastic Nylon PA66 · Density: typicalPlastic Nylon PA66 · Thermal conductivity: typicalPlastic Nylon PA66 · Thermal expansion: longitudinal, 23-55 °CPlastic Nylon PA66 · Specific heat: typicalPlastic Nylon PA66 · Melting point: DSCPlastic Nylon PA66 · Max service temperature: IEC 60216 temperature index, 20000 h
- 3RenAM 500 Series Aluminium AlSi10Mg Material Data SheetRenishawDMLS AlSi10Mg Aluminum · Young's modulus (stiffness): same material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
- 4EOS Aluminium AlSi10Mg Material Data Sheet, FlexLine, M 290 (2018)EOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Density: typical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
- 5MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseDMLS AlSi10Mg Aluminum · Poisson's ratio: base material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)DMLS AlSi10Mg Aluminum · Specific heat: base material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C
- 6Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA66 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS AlSi10Mg Aluminum is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS AlSi10Mg Aluminum stronger than Plastic Nylon PA66?
DMLS AlSi10Mg Aluminum is stronger: its yield strength is 270 MPa against 85 MPa for Plastic Nylon PA66 (3.18x).
Which is lighter, DMLS AlSi10Mg Aluminum or Plastic Nylon PA66?
Plastic Nylon PA66 is lighter: 1,130 kg/m³ against 2,670 kg/m³ for DMLS AlSi10Mg Aluminum.
Which is stiffer, DMLS AlSi10Mg Aluminum or Plastic Nylon PA66?
DMLS AlSi10Mg Aluminum is stiffer: Young's modulus 72 GPa against 3 GPa for Plastic Nylon PA66, so the same part in DMLS AlSi10Mg Aluminum deflects less under the same load.
Which is lighter for the same job, DMLS AlSi10Mg Aluminum or Plastic Nylon PA66?
For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie; Plastic Nylon PA66 is lighter for a strong beam, strong panel or plate.
| Part that must be | DMLS AlSi10Mg Aluminum | Plastic Nylon PA66 |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 10.2x heavier |
| Stiff beam (bending) | lighter | 2.07x heavier |
| Stiff panel or plate | lighter | 22% heavier |
| Strong rod or tie | lighter | 34% heavier |
| Strong beam | 9% heavier | lighter |
| Strong panel or plate | 33% heavier | lighter |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, DMLS AlSi10Mg Aluminum or Plastic Nylon PA66?
Plastic Nylon PA66 stretches further before it breaks: 30% elongation at break against 10.2% for DMLS AlSi10Mg Aluminum.
Thermal
Which conducts heat better, DMLS AlSi10Mg Aluminum or Plastic Nylon PA66?
DMLS AlSi10Mg Aluminum conducts heat better: 110 W/m·K against 0.33 W/m·K for Plastic Nylon PA66.
Which expands less with temperature?
DMLS AlSi10Mg Aluminum expands less: 20 µm/m·K against 98 µm/m·K for Plastic Nylon PA66.
Related comparisons
- DMLS AlSi10Mg Aluminum vs. Aluminum
- DMLS AlSi10Mg Aluminum vs. Aluminum 6061-T6
- DMLS AlSi10Mg Aluminum vs. Aluminum 2024-T351
- DMLS AlSi10Mg Aluminum vs. Aluminum 6063-T6
- Plastic Nylon PA66 vs. Plastic PMMA
- Plastic Nylon PA66 vs. Plastic Nylon PA6
- Plastic Nylon PA66 vs. FDM PAHT-CF
- Plastic Nylon PA66 vs. Plastic POM/Acetal