Materials / Compare
DMLS AlSi10Mg Aluminum vs. Plastic PLA
Compare DMLS AlSi10Mg Aluminum vs. Plastic PLA strength, stiffness, weight and thermal properties.
| Mechanical | DMLS AlSi10Mg Aluminum | Plastic PLA |
|---|---|---|
| Yield strength | 270MPa15.14x stronger | 52.5MPa2 |
| Ultimate tensile strength | 450MPa18.57x stronger | 52.5MPa2 |
| Flexural strength | not sourced | 96.8MPa2 |
| Elongation at break | 10.2%131% more ductile | 7.8%2 |
| Young's modulus (stiffness) | 72GPa322.2x stiffer | 3.25GPa2 |
| Density | 2,670kg/m³4 | 1,240kg/m³22.15x lighter |
| Strength to weight | 101kN·m/kg2.39x higher | 42.3kN·m/kg |
| Stiffness to weight | 27MN·m/kg10.3x higher | 2.62MN·m/kg |
| Poisson's ratio | base material0.335 | not sourced |
| Shear modulus | 27.1GPa | not sourced |
| Bulk modulus | 70.6GPa | not sourced |
| Speed of sound | 5,193m/s3.21x faster | 1,619m/s |
| Thermal | DMLS AlSi10Mg Aluminum | Plastic PLA |
|---|---|---|
| Thermal conductivity | 110W/m·K1846x more heat through a fin | base material0.13W/m·K6 |
| Thermal expansion | mean 25-100 °C20µm/m·K1 | not sourced |
| 100 mm part over a 50 °C swing | 100µm growth | not sourced |
| Specific heat | base material963J/kg·K5 | base material1,200J/kg·K6 |
| Heats up and cools (diffusivity) | 42.8mm²/s490x faster | 0.0874mm²/s |
| Thermal shock resistance | 13,819W/m | not sourced |
| Melting point | not sourced | 152°C2 |
| Glass transition | not sourced | 59.1°C2 |
| Max service temperature | not sourced | HDT 0.455 MPa58.8°C2 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources6 documents: EOS GmbH, UltiMaker, Renishaw, U.S. Department of Defense, NatureWorks
- DMLS AlSi10Mg Aluminum
- EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10
- Plastic PLA
- Ultimaker PLA, 3D-printed specimens, XY (flat) orientation; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS dated April 20, 2022.
- 1EOS Aluminium AlSi10Mg Material Data SheetEOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Yield strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Ultimate tensile strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Elongation at break: typical at break, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Thermal conductivity: typical, as manufactured, horizontal (ISO 22007-2)DMLS AlSi10Mg Aluminum · Thermal expansion: mean 25-100 °C, ASTM E228
- 2Ultimaker PLA Technical Data Sheet, v5.00UltiMakerarchived copyPlastic PLA · Yield strength: typicalPlastic PLA · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic PLA · Flexural strength: typicalPlastic PLA · Elongation at break: typicalPlastic PLA · Young's modulus (stiffness): typicalPlastic PLA · Density: typicalPlastic PLA · Melting point: typicalPlastic PLA · Glass transition: typicalPlastic PLA · Max service temperature: HDT 0.455 MPa (printed specimens)
- 3RenAM 500 Series Aluminium AlSi10Mg Material Data SheetRenishawDMLS AlSi10Mg Aluminum · Young's modulus (stiffness): same material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
- 4EOS Aluminium AlSi10Mg Material Data Sheet, FlexLine, M 290 (2018)EOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Density: typical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
- 5MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseDMLS AlSi10Mg Aluminum · Poisson's ratio: base material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)DMLS AlSi10Mg Aluminum · Specific heat: base material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C
- 6Engineering Properties of Ingeo BiopolymerNatureWorksarchived copyPlastic PLA · Thermal conductivity: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °CPlastic PLA · Specific heat: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS AlSi10Mg Aluminum and Plastic PLA are 3D printed: their properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS AlSi10Mg Aluminum stronger than Plastic PLA?
DMLS AlSi10Mg Aluminum is stronger: its yield strength is 270 MPa against 52.5 MPa for Plastic PLA (5.14x).
Which is lighter, DMLS AlSi10Mg Aluminum or Plastic PLA?
Plastic PLA is lighter: 1,240 kg/m³ against 2,670 kg/m³ for DMLS AlSi10Mg Aluminum.
Which is stiffer, DMLS AlSi10Mg Aluminum or Plastic PLA?
DMLS AlSi10Mg Aluminum is stiffer: Young's modulus 72 GPa against 3.25 GPa for Plastic PLA, so the same part in DMLS AlSi10Mg Aluminum deflects less under the same load.
Which is lighter for the same job, DMLS AlSi10Mg Aluminum or Plastic PLA?
For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
| Part that must be | DMLS AlSi10Mg Aluminum | Plastic PLA |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 10.3x heavier |
| Stiff beam (bending) | lighter | 2.19x heavier |
| Stiff panel or plate | lighter | 30% heavier |
| Strong rod or tie | lighter | 2.39x heavier |
| Strong beam | lighter | 38% heavier |
| Strong panel or plate | lighter | 5% heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, DMLS AlSi10Mg Aluminum or Plastic PLA?
DMLS AlSi10Mg Aluminum stretches further before it breaks: 10.2% elongation at break against 7.8% for Plastic PLA.
Thermal
Which conducts heat better, DMLS AlSi10Mg Aluminum or Plastic PLA?
DMLS AlSi10Mg Aluminum conducts heat better: 110 W/m·K against 0.13 W/m·K for Plastic PLA.
Related comparisons
- DMLS AlSi10Mg Aluminum vs. Aluminum
- DMLS AlSi10Mg Aluminum vs. Aluminum 6061-T6
- DMLS AlSi10Mg Aluminum vs. Aluminum 2024-T351
- DMLS AlSi10Mg Aluminum vs. Aluminum 6063-T6
- Plastic PLA vs. SLA Resin Standard
- Plastic PLA vs. FDM Polycarbonate
- Plastic PLA vs. Plastic POM/Acetal
- Plastic PLA vs. Plastic Polycarbonate