Materials / Compare
DMLS AlSi10Mg Aluminum vs. Plastic Polycarbonate
Compare DMLS AlSi10Mg Aluminum vs. Plastic Polycarbonate strength, stiffness, weight and thermal properties.
| Mechanical | DMLS AlSi10Mg Aluminum | Plastic Polycarbonate |
|---|---|---|
| Yield strength | 270MPa14.15x stronger | 65MPa2 |
| Ultimate tensile strength | 450MPa1 | 65MPa2 |
| Flexural strength | not sourced | 97MPa2 |
| Elongation at break | 10.2%1 | 125%212.3x more ductile |
| Young's modulus (stiffness) | 72GPa330x stiffer | 2.4GPa2 |
| Density | 2,670kg/m³4 | 1,200kg/m³22.23x lighter |
| Strength to weight | 101kN·m/kg1.87x higher | 54.2kN·m/kg |
| Stiffness to weight | 27MN·m/kg13.5x higher | 2MN·m/kg |
| Poisson's ratio | base material0.335 | 0.386 |
| Shear modulus | 27.1GPa31.1x stiffer in shear | 0.87GPa |
| Bulk modulus | 70.6GPa21.2x higher | 3.33GPa |
| Speed of sound | 5,193m/s3.67x faster | 1,414m/s |
| Thermal | DMLS AlSi10Mg Aluminum | Plastic Polycarbonate |
|---|---|---|
| Thermal conductivity | 110W/m·K1550x more heat through a fin | 0.2W/m·K2 |
| Thermal expansion | mean 25-100 °C20µm/m·K13.25x less | 65µm/m·K2 |
| 100 mm part over a 50 °C swing | 100µm growth3.25x less | 325µm growth |
| Specific heat | base material963J/kg·K5 | 1,172J/kg·K7 |
| Heats up and cools (diffusivity) | 42.8mm²/s301x faster | 0.142mm²/s |
| Thermal shock resistance | 13,819W/m267x more resistant | 51.7W/m |
| Glass transition | not sourced | 144°C2 |
| Max service temperature | not sourced | UL 746B RTI125°C2 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources7 documents: EOS GmbH, Covestro, Renishaw, U.S. Department of Defense, Bayer MaterialScience
- DMLS AlSi10Mg Aluminum
- EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10
- Plastic Polycarbonate
- Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values
- 1EOS Aluminium AlSi10Mg Material Data SheetEOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Yield strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Ultimate tensile strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Elongation at break: typical at break, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Thermal conductivity: typical, as manufactured, horizontal (ISO 22007-2)DMLS AlSi10Mg Aluminum · Thermal expansion: mean 25-100 °C, ASTM E228
- 2Makrolon 2405 Technical Data SheetCovestroPlastic Polycarbonate · Yield strength: typical, tensile yieldPlastic Polycarbonate · Ultimate tensile strength: typical, stress at breakPlastic Polycarbonate · Flexural strength: typical, flexural strengthPlastic Polycarbonate · Elongation at break: typical, strain at breakPlastic Polycarbonate · Young's modulus (stiffness): typicalPlastic Polycarbonate · Density: typicalPlastic Polycarbonate · Thermal conductivity: typical, through-plane, 23 CPlastic Polycarbonate · Thermal expansion: typical, 23-55 C, parallel and normalPlastic Polycarbonate · Glass transition: typical, DSC 10 C/minPlastic Polycarbonate · Max service temperature: UL 746B RTI, tensile strength, 1.5 mm
- 3RenAM 500 Series Aluminium AlSi10Mg Material Data SheetRenishawDMLS AlSi10Mg Aluminum · Young's modulus (stiffness): same material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
- 4EOS Aluminium AlSi10Mg Material Data Sheet, FlexLine, M 290 (2018)EOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Density: typical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
- 5MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseDMLS AlSi10Mg Aluminum · Poisson's ratio: base material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)DMLS AlSi10Mg Aluminum · Specific heat: base material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C
- 6Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
- 7Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS AlSi10Mg Aluminum is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS AlSi10Mg Aluminum stronger than Plastic Polycarbonate?
DMLS AlSi10Mg Aluminum is stronger: its yield strength is 270 MPa against 65 MPa for Plastic Polycarbonate (4.15x).
Which is lighter, DMLS AlSi10Mg Aluminum or Plastic Polycarbonate?
Plastic Polycarbonate is lighter: 1,200 kg/m³ against 2,670 kg/m³ for DMLS AlSi10Mg Aluminum.
Which is stiffer, DMLS AlSi10Mg Aluminum or Plastic Polycarbonate?
DMLS AlSi10Mg Aluminum is stiffer: Young's modulus 72 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in DMLS AlSi10Mg Aluminum deflects less under the same load.
Which is lighter for the same job, DMLS AlSi10Mg Aluminum or Plastic Polycarbonate?
For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam; Plastic Polycarbonate is lighter for a strong panel or plate.
| Part that must be | DMLS AlSi10Mg Aluminum | Plastic Polycarbonate |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 13.5x heavier |
| Stiff beam (bending) | lighter | 2.46x heavier |
| Stiff panel or plate | lighter | 40% heavier |
| Strong rod or tie | lighter | 1.87x heavier |
| Strong beam | lighter | 16% heavier |
| Strong panel or plate | 9% heavier | lighter |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, DMLS AlSi10Mg Aluminum or Plastic Polycarbonate?
Plastic Polycarbonate stretches further before it breaks: 125% elongation at break against 10.2% for DMLS AlSi10Mg Aluminum.
Thermal
Which conducts heat better, DMLS AlSi10Mg Aluminum or Plastic Polycarbonate?
DMLS AlSi10Mg Aluminum conducts heat better: 110 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.
Which expands less with temperature?
DMLS AlSi10Mg Aluminum expands less: 20 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.
Related comparisons
- DMLS AlSi10Mg Aluminum vs. Aluminum
- DMLS AlSi10Mg Aluminum vs. Aluminum 6061-T6
- DMLS AlSi10Mg Aluminum vs. Aluminum 2024-T351
- DMLS AlSi10Mg Aluminum vs. Aluminum 6063-T6
- Plastic Polycarbonate vs. Plastic Nylon
- Plastic Polycarbonate vs. SLA Resin Standard
- Plastic Polycarbonate vs. FDM Polycarbonate
- Plastic Polycarbonate vs. Plastic POM/Acetal