Materials / Compare
DMLS AlSi10Mg Aluminum vs. Titanium Ti-6Al-4V
Compare DMLS AlSi10Mg Aluminum vs. Titanium Ti-6Al-4V strength, stiffness, weight and thermal properties.
| Mechanical | DMLS AlSi10Mg Aluminum | Titanium Ti-6Al-4V |
|---|---|---|
| Yield strength | 270MPa1 | 885MPa23.28x stronger |
| Ultimate tensile strength | 450MPa1 | 940MPa22.09x stronger |
| Elongation at break | 10.2%1 | 16%21.57x more ductile |
| Young's modulus (stiffness) | 72GPa3 | 107–122GPa4 |
| Density | 2,670kg/m³51.66x lighter | 4,430kg/m³2 |
| Strength to weight | 101kN·m/kg | 200kN·m/kg1.98x higher |
| Stiffness to weight | 27MN·m/kg4% higher | 25.8MN·m/kg |
| Poisson's ratio | base material0.336 | 0.3422 |
| Shear modulus | 27.1GPa | 42.7GPa1.58x stiffer in shear |
| Bulk modulus | 70.6GPa | 121GPa1.71x higher |
| Speed of sound | 5,193m/s2% faster | 5,084m/s |
| Thermal | DMLS AlSi10Mg Aluminum | Titanium Ti-6Al-4V |
|---|---|---|
| Thermal conductivity | 110W/m·K116.7x more heat through a fin | 6.6W/m·K4 |
| Thermal expansion | mean 25-100 °C20µm/m·K1 | 9µm/m·K42.22x less |
| 100 mm part over a 50 °C swing | 100µm growth | 45µm growth2.22x less |
| Specific heat | base material963J/kg·K6 | 580J/kg·K4 |
| Heats up and cools (diffusivity) | 42.8mm²/s16.7x faster | 2.57mm²/s |
| Thermal shock resistance | 13,819W/m3.71x more resistant | 3,730W/m |
| Melting point | not sourced | melting range1,630–1,650°C2 |
| Max service temperature | not sourced | 400°C2 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources6 documents: EOS GmbH, TIMET, Renishaw, U.S. Department of Defense
- DMLS AlSi10Mg Aluminum
- EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10
- Titanium Ti-6Al-4V
- TIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties
- 1EOS Aluminium AlSi10Mg Material Data SheetEOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Yield strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Ultimate tensile strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Elongation at break: typical at break, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Thermal conductivity: typical, as manufactured, horizontal (ISO 22007-2)DMLS AlSi10Mg Aluminum · Thermal expansion: mean 25-100 °C, ASTM E228
- 2TIMETAL 6-4 PropertiesTIMETarchived copyTitanium Ti-6Al-4V · Yield strength: typical, plate (>0.187 in), annealed, 0.2% offsetTitanium Ti-6Al-4V · Ultimate tensile strength: typical, plate, annealedTitanium Ti-6Al-4V · Elongation at break: typical, in 2 in., plate annealedTitanium Ti-6Al-4V · Density: nominalTitanium Ti-6Al-4V · Poisson's ratio: mean of TIMET measurementsTitanium Ti-6Al-4V · Melting point: melting rangeTitanium Ti-6Al-4V · Max service temperature: upper recommended use temperature
- 3RenAM 500 Series Aluminium AlSi10Mg Material Data SheetRenishawDMLS AlSi10Mg Aluminum · Young's modulus (stiffness): same material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
- 4TIMETAL 6-4 Data SheetTIMETarchived copyTitanium Ti-6Al-4V · Young's modulus (stiffness): typical range, 20 °CTitanium Ti-6Al-4V · Thermal conductivity: typical, 20 °C, mill annealedTitanium Ti-6Al-4V · Thermal expansion: typical, mean 0-100 °CTitanium Ti-6Al-4V · Specific heat: typical, 20 °C
- 5EOS Aluminium AlSi10Mg Material Data Sheet, FlexLine, M 290 (2018)EOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Density: typical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
- 6MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseDMLS AlSi10Mg Aluminum · Poisson's ratio: base material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)DMLS AlSi10Mg Aluminum · Specific heat: base material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS AlSi10Mg Aluminum is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS AlSi10Mg Aluminum stronger than Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V is stronger: its yield strength is 885 MPa against 270 MPa for DMLS AlSi10Mg Aluminum (3.28x).
Which is lighter, DMLS AlSi10Mg Aluminum or Titanium Ti-6Al-4V?
DMLS AlSi10Mg Aluminum is lighter: 2,670 kg/m³ against 4,430 kg/m³ for Titanium Ti-6Al-4V.
Which is stiffer, DMLS AlSi10Mg Aluminum or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V is stiffer: Young's modulus 115 GPa against 72 GPa for DMLS AlSi10Mg Aluminum, so the same part in Titanium Ti-6Al-4V deflects less under the same load.
Which is lighter for the same job, DMLS AlSi10Mg Aluminum or Titanium Ti-6Al-4V?
For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Titanium Ti-6Al-4V is lighter for a strong rod or tie, strong beam, strong panel or plate.
| Part that must be | DMLS AlSi10Mg Aluminum | Titanium Ti-6Al-4V |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 4% heavier |
| Stiff beam (bending) | lighter | 32% heavier |
| Stiff panel or plate | lighter | 42% heavier |
| Strong rod or tie | 1.98x heavier | lighter |
| Strong beam | 33% heavier | lighter |
| Strong panel or plate | 9% heavier | lighter |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, DMLS AlSi10Mg Aluminum or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V stretches further before it breaks: 16% elongation at break against 10.2% for DMLS AlSi10Mg Aluminum.
Thermal
Which conducts heat better, DMLS AlSi10Mg Aluminum or Titanium Ti-6Al-4V?
DMLS AlSi10Mg Aluminum conducts heat better: 110 W/m·K against 6.6 W/m·K for Titanium Ti-6Al-4V.
Which expands less with temperature?
Titanium Ti-6Al-4V expands less: 9 µm/m·K against 20 µm/m·K for DMLS AlSi10Mg Aluminum.
Related comparisons
- DMLS AlSi10Mg Aluminum vs. Aluminum
- DMLS AlSi10Mg Aluminum vs. Aluminum 6061-T6
- DMLS AlSi10Mg Aluminum vs. Aluminum 2024-T351
- DMLS AlSi10Mg Aluminum vs. Aluminum 6063-T6
- Titanium Ti-6Al-4V vs. Titanium
- Titanium Ti-6Al-4V vs. DMLS Ti-6Al-4V ELI Titanium
- Titanium Ti-6Al-4V vs. DMLS 17-4PH Stainless Steel
- Titanium Ti-6Al-4V vs. Steel AISI 4340